MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
3M Dyneon™ FE 5542X Fluoroelastomer  (discontinued **)
Categories: Polymer; Thermoset; Fluoropolymer, TS; Rubber or Thermoset Elastomer (TSE)

Material Notes:
  • Composition: Low fluorine content terpolymer of vinylidene fluoride, hexafluoropropylene, and tetrafluoroethylene
  • Medium viscosity gum stock without incorporated curatives
  • Process targets: Transfer and compression molding, extrusion, calendering
  • FE 5542X is amine or bisphenol curable
  • Improved low temperature flexibility over standard dipolymers and terpolymers

Information provided by Dyneon, A 3M Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.80 g/cc
Mooney Viscosity 42
@Temperature 121 °C
ML1+10
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 75Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C; ASTM D2240
Tensile Strength at Break 2100 psiPress Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C
Elongation at Break 180 %Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C
100% Modulus 1.00 ksi
@Strain 100 %
Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C
Compression Set 18 %
@Temperature 200 °C,
Time 252000 sec
 
Thermal PropertiesOriginal ValueComments
Transformation Temperature -19.0 °CTR10; ASTM D1329
 
Component Elements PropertiesOriginal ValueComments
Fluorine, F 65.5 %
 
Descriptive Properties
5`50, Time to 50% cure, minutes1.8177°C
ColorTranslucent to Off-White
MH, Maximum Torque, inch-lb @ 177°C22
ML, Minimum Torque inch-lb @ 177°C1.5
SolubilityKetones and Esters
t`90 - Time to 90% cure @ 177°C - minutes2.4
ts2 - Time to 2 in-lb rise from min @ 177°C - min1.5

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Avient Dynaflex™ G7970-9001-02 Thermoplastic Elastomer (TPE)
Avient Dynaflex™ G7970-1001-00 Thermoplastic Elastomer (TPE)
ATG s.r.l. EPM Ethylene-Propylene Copolymer
ATG s.r.l. EPDM Ethylene-Propylene Terpolymer
AGC AFLAS® SZ TFE/P/VdF Fluoroelastomer

PDYNE122 / 34930

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.