MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SABIC LNP™ STAT-KON™ Compound DX13301C Polycarbonate (PC)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: LNP STAT-KON DX13301C compound is based on Polycarbonate (PC) resin containing proprietary fillers. Added features of this grade include: Electrically Conductive, LNP Clean Compounding Technology.

Features: LNP Clean Compound Technology,Electrically Conductive

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.25 g/ccASTM D792
Density 1.25 g/ccASTM D792
Moisture Absorption 0.0200 %Injection Molding
 0.150 %23°C/50% RH/24 hrs; ASTM D570
 0.230 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0074 cm/cm24hrs; ASTM D955
Linear Mold Shrinkage, Transverse 0.0085 cm/cm24hrs; ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 54.0 MPa5 mm/min; ASTM D638
 54.0 MPa5 mm/min; ISO 527
Tensile Strength, Yield 63.0 MPa5 mm/min; ISO 527
 64.0 MPa5 mm/min; ASTM D638
Elongation at Break 20 %5 mm/min; ASTM D638
 20 %5 mm/min; ISO 527
Elongation at Yield 4.9 %5 mm/min; ASTM D638
 4.9 %5 mm/min; ISO 527
Tensile Modulus 2910 MPa1 mm/min; ISO 527
 3000 MPa5 mm/min; ASTM D638
Flexural Strength 100 MPaISO 178
Flexural Modulus 2770 MPaISO 178
 2890 MPaASTM D790
Izod Impact Notched 61.0 JASTM D256
Izod Impact, Unnotched NBASTM D4812
Izod Impact, Notched (ISO) 7.50 kJ/m²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) NB80*10*4; ISO 180/1U
Dart Drop, Total Energy 41.0 JASTM D3763
Impact Test 38.0 JMultiaxial Impact; ISO 6603
 
Electrical PropertiesOriginal ValueComments
Surface Resistance 100 - 1.00e+6 ohmASTM D257
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 62.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
ASTM E831
CTE, linear, Transverse to Flow 63.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 142 °CFlatw 80*10*4 sp=64mm; ISO 75/Bf
 142 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 131 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 133 °C
@Thickness 3.20 mm
unannealed; ASTM D648
 
Processing PropertiesOriginal ValueComments
Zone 2 310 - 321 °C
Zone 3 321 - 332 °C
Melt Temperature 304 - 326 °CInjection Molding
Mold Temperature 82.0 - 110 °C
Drying Temperature 121 °CInjection Molding
Dry Time 4.00 hourInjection Molding
Back Pressure 0.170 - 0.340 MPa
Screw Speed 30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH81266 / 289213

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.