MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
SCG Chemicals P686J Impact copolymer polypropylene resin
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Impact Modified; Molded/Extruded

Material Notes: SCG PP P686J is an impact copolymer polypropylene resin which contains nucleating agent. It is designed for injection molding process. This resin recommended for product that requires high strength with high stiffness and good productivity.

Application: Pail, crate, container, Automotive parts, Electrical appliance parts, Industrial parts.

Features: High impact strength. High stiffness. Good productivity.

Information provided by SCG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.910 g/ccASTM D 1505
Linear Mold Shrinkage, Flow 0.013 in/in
@Thickness 2.00 mm
TPE Method
Linear Mold Shrinkage, Transverse 0.013 in/in
@Thickness 2.00 mm
TPE Method
Melt Flow 10 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 60ASTM D785
Tensile Strength at Break 24.5 MPaCrosshead speed 50 mm/min; ASTM D638
Tensile Strength, Yield 28.4 MPaCrosshead speed 50 mm/min; ASTM D638
Flexural Modulus 1320 MPaASTM D790
Izod Impact, Notched 50.0 J/m
@Temperature -20.0 °C
ASTM D256
 80.0 J/m
@Temperature 0.000 °C
ASTM D256
 120 J/m
@Temperature 23.0 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Melting Point 163 °CASTM D2117
Deflection Temperature at 0.46 MPa (66 psi) 115 °CASTM D648
 
Descriptive Properties
AppearancePellet

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSCGC771 / 278028

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.