MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

(Viewing data as-entered. Click here to return)
Johnson Matthey Pallabraze™ 1090 Palladium Based Brazing Alloy
Categories: Metal; Nonferrous Metal; Copper Alloy; Solder/Braze Alloy

Material Notes: Joints brazed Johnson Matthey’s Pallabraze alloys have good oxidation resistance and improved mechanical strength at elevated temperatures over standard silver brazing alloys. Pallabraze alloys offer good corrosion resistance in many environments. They show resistance to interfacial corrosion when brazing ferritic and austenitic stainless steels. Palladium-bearing alloys do not cause ‘stress cracking' and are recommended on iron-nickel-cobalt alloys. Pallabrazes have excellent flow and penetration qualities but are also capable of filling joint gaps up to 0.5mm.

Typical applications are for brazing thermionic valve devices and aerospace components. Pallabraze alloys have been used in the glass and chemical industries where increased resistance to corrosion and chemical attack makes them a good choice. It can be used to join copper, stainless steel, super alloys, nickel, iron, cobalt, molybdenum, niobium, tungsten and their alloys. Grade V1 is normally used for components that see service in vacuum.

Information provided by Johnson Matthey Metal Joining

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesOriginal ValueComments
Melting Point 1080 - 1090 °C
Solidus 1080 °C
Liquidus 1090 °C
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 82 %
Palladium, Pd 18 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
1070 Aluminum Composition Spec
Indium Corp. Indalloy® 151 Pb-Sn-Ag Solder Alloy
Johnson Matthey Pallabraze™ 1070 Precious Metal Brazing Filler Metal
Indium Corp. Indalloy® 256 96.5Sn/3.0Ag/0.5Cu Lead-Free Solder Alloy
ChevronTexaco Texcool® P 200

NJMMJ9748 / 186149

solder replacement adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.