MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Hyflon® MFA® D 5510 Perfluoropolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Fluoropolymer; TFE/Perfluoromethylvinylether Copolymer (MFA)

Material Notes: Hyflon® MFA® D 5510 is a white aqueous MFA dispersion. Hyflon® MFA® D 5510 exhibits excellent wetting properties and high shear stability. Hyflon® MFA® D 5510 has very good film forming behavior and is especially suited for top-coat passes to produce final items with superior gloss. Due to its features, D 5100 can of course also find use in formulations for coating applications. Main features of Hyflon® MFA® D 5510 dispersion are:
  • No polyethoxylated alkylphenols
  • Excellent wetting properties
  • Superior gloss of final items.

Availability:

  • Africa & Middle East
  • Asia Pacific
  • Europe
  • Latin America
  • North America
Features:
  • High Gloss
  • Rapid Wetting
Uses:
  • Impregnation Applications
  • Coating Applications
Forms: Liquid

Information provided by Solvay

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.41 g/ccASTM D4441
Particle Size 180 µmAverage
pH >= 9.0ASTM D4441
Brookfield Viscosity 20 cPASTM D2196
 
Thermal PropertiesOriginal ValueComments
Melting Point 310 °CASTM D4591
 
Descriptive Properties
AppearanceWhite
Content3.5%Non Ionic Surfactant, ASTM D4441
 55%MFA, ASTM D4441

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSOLVAY521 / 218249

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.