MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Imerys Kaolex™ SC Kaolin
Categories: Ceramic; Clay; Kaolin Clay

Material Notes: Kaolex SC is an air floated Hydrated Aluminum Silicate. It is a low surface area, low viscosity, medium casting filler/extender for ceramic applications.

Information provided by Imerys

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.60 g/cc
Oil Absorption 200 - 300 %g/100g clay; rub out method
Particle Size 1.1 µmaverage
Particle Mesh Size 325 Mesh1.01% retained
pH 4.0 - 5.528%
Specific Surface Area 12 - 15 m²/g
Brookfield Viscosity >= 100 cP
@Temperature 25.0 °C
20 RPM, 70% clay/water slip
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity <= 0.100 ohm-cmspecific resistance
 
Component Elements PropertiesOriginal ValueComments
H2O, Water <= 2.0 %
@Temperature 105 °C
as produced
 
Descriptive Properties
Colorwhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

CIMERY043 / 88393

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.