MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Clariant PBTSP0008WT-199 Polybutylene Terephthalate, Glass Reinforced, Flame Retardant  (discontinued **)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant

Material Notes:

Data provided by Clariant Masterbatches

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.66 g/ccASTM D792
Filler Content 30 %ASTM D2584
Linear Mold Shrinkage, Flow 0.0030 - 0.0050 in/inASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 17500 psiASTM D638
Elongation at Yield 3.0 %ASTM D638
Flexural Yield Strength 24000 psiASTM D790
Flexural Modulus 1.30e+6 psiASTM D790
Izod Impact, Notched 1.20 ft-lb/in
@Temperature 22.8 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 415 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 390 °FASTM D648
Flammability, UL94 V-01/32, 1/16, 1/8, 1/4
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 430 - 480 °F
Middle Barrel Temperature 440 - 490 °F
Front Barrel Temperature 450 - 500 °F
Nozzle Temperature 460 - 510 °F
Melt Temperature 450 - 500 °F
Mold Temperature 180 - 250 °F
Dry Time <= 4 hourto ensure the moisture level is less than 0.02%
Injection Pressure 720 - 1200 psiSecondary
 1200 - 2000 psiInitial
Back Pressure 50.0 psi
Shot Size 30 - 80 %
Screw Speed 25 - 100 rpm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant
PTS PBT-1100 PBT Resin
PTS 15GFR-BK PBT- Flame Retardant, 15% Glass Filled PBT Black Resin
E-Polymers TEKASTER® F10G30FR 30% Glass Fiber Reinforced Flame Retardant PBT
Edinburg Plastics BTG066 PBT Flame Retardant, 8% Glass Filled

PCLAR145 / 82270

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.