MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
I. Stern IS-7985 Polyethylene Terephthalate Resin  (discontinued **)
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), Unreinforced

Material Notes: Product Description: IS-7985 is a natural polyethylene terephthalate (PET) resin. This resin is produced by continuous melt phase polymerization followed by solid phase polymerization.

Certification: IS-7985 is ideally suited for food packaging applications and is considered in compliance with the Food and Drug Administration (FDA) Food Additive Regulation 21 CFR 177.1630, covering PET polymers.

Information provided by I. Stern & Co. Inc.

I. Stern & Co. Inc. has been acquired by Ravago.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 54.3 lb/ft³C-186
Density >= 1.39 g/ccC-2011
Viscosity Measurement 0.79 - 0.80Intrinsic Viscosity; C-100a
 
Chemical PropertiesOriginal ValueComments
Acetaldehyde <= 3.00 ppmC-170b
 
Thermal PropertiesOriginal ValueComments
Melting Point 240 °CC-120
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.
 
Descriptive Properties
Color "b"-2 ± 6.0Hunter, C-111
Color "L"78.0 ± 8.0Hunter, C-111
Nominal Chip Size34 to 74 chips per gramC-185

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Indorama AlphaPet Preformance® 1708CC(A) PET Resin
Iran Petrochemical (PCC) PET BG-821 Polyethylene Terephthalate
Intercontinental Polymers 1180 Bicomponent PP/PET Fiber Type - 3 Denier X 1.5 Inches
Intercontinental Polymers 169 PET Polymer Type - Cationic, Semi-Dull, Polyester Pellets
Intercontinental Polymers HoPET 737 Bright, Polyester Pellets

PISTER930 / 130890

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.