MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese Celanex® 6402R PBT, 40% Mineral / Glass Reinforced
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Glass + Mineral Filled

Material Notes: Celanex 6402R is a 40% Glass/ mineral filled polyester with 25% Post Consumer Recycled content. It is available in natural, black and various colors including metallic colors.

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.66 g/ccISO 1183
Linear Mold Shrinkage, Flow 0.0010 cm/cmISO 294-4
Linear Mold Shrinkage, Transverse 0.0050 cm/cmISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 147 MPa5mm/min; ISO 527-2/1A
Elongation at Break 2.1 %5mm/min; ISO 527-2/1A
Tensile Modulus 13500 MPa50mm/min; ISO 527-2/1A
Flexural Strength 220 MPaISO 178
Flexural Modulus 12500 MPaISO 178
Izod Impact, Notched 1.30 ft-lb/inASTM D256
 1.60 ft-lb/in
@Temperature -30.0 °C
ASTM D256
Charpy Impact, Notched 7.50 kJ/m²ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 205 °CISO 75-1, -2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Celanex® 4306 PBT, 30% Glass Reinforced
Asahi Kasei Thermylene® P6-30FG-0600 30% Glass Fiber Reinforced, Heat Stabilized Polypropylene
Celanese Celanex® 733LD PBT, Glass Reinforced
Celanese Celstran® PP-GF40-20 AD 3004 Black PP, 40% Glass Reinforced
Covestro Makrolon® 2607 Polycarbonate, Injection Grade

PHCQ082 / 178537

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.