MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ChevronTexaco 1000 THF Tractor Hydraulic Fluid
Categories: Fluid; Lubricant

Material Notes: Chevron 1000 THF (formerly Chevron Tractor Hydraulic Fluid and Amoco 1000 Fluid) is a high quality, multifunctional fluid, specially formulated for use in transmissions, final drives, wet brakes, and hydraulic systems of tractors and other equipment employing a common fluid reservoir.

It is formulated with ISOSYN™ base stocks, a viscosity index improver, oxidation and corrosion inhibitors, antiwear and film strength additives, an antifoaming agent, and a pour point depressant.

Its distinctive orange color allows for easy product identification and leak detection.

Chevron 1000 THF is recommended for use as a mutifunctional fluid in all types of farm tractors an equipment. It can be used in any application which calls for the following OEM lubricant specifications:

  • AGCO-improved power fluid 821XL
  • John Deere-J20C
  • Ford New Holland-ESN-<2C134-D, FNHA 2 C 201
  • Massey Ferguson-M1135, M1141, M1143
  • White Farm Equipment-Q-1826
  • Case Corporation-JIC-143, JIC-145, MS 1206, MS 1207, MS 1209, MS 1210 (TCH)
  • Oliver-Type 55
  • Minneapolis-Moline-Fluids
  • Caterpillar-TO-2, MTO
  • Renk-Bus Automatic Transmission Fluid
  • Kubota-UDT
  • International Harvester-B6
  • VolvoWB 101

Key Words: CPS Number: 226606; MSDS Number: 7648
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
API Gravity 29.9 °
Brookfield Viscosity 40000 cP
@Temperature -35.0 °C
Viscosity Measurement 145Viscosity Index; ASTM D2270
Saybolt Viscosity at 100°F 298 SUS
Saybolt Viscosity at 210°F 58.3 SUS
Kinematic Viscosity at 40°C (104°F) 58.4 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 9.5 cStASTM D445
 
Thermal PropertiesOriginal ValueComments
Pour Point -42.0 °CASTM D97
Flash Point 235 °CASTM D92
 
Descriptive Properties
ColorOrange

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow 1410 ANTIFOAM
Honeywell TLP-2020 Lubricant Blend
ChevronTexaco 120 Aircraft Engine Oils
ChevronTexaco 10-T White Oil
ChevronTexaco 100 White Oil

WCHEV038 / 74653

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.