MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Master Bond Supreme 10HT One Component, Low Outgassing, Toughened Epoxy System
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Master Bond Supreme 10HT features a unique blend of performance properties including both high shear and peel strengths along with convenient handling. Supreme 10HT is room temperature storable and its working life is unlimited at room temperature. This epoxy is cryogenically serviceable and has a wide temperature range of 4K to +400°F.

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Viscosity >= 250000 cP
@Temperature 23.0 °C
Storage Temperature 75.0 °F6 months
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 400 °F
Minimum Service Temperature, Air -453 °F
 
Processing PropertiesOriginal ValueComments
Cure Time 0.750 hour
@Temperature 149 °C
 1.00 hour
@Temperature 121 °C
 
Descriptive Properties
ColorGray

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Master Bond EP30AN-1 Low Viscosity, NASA Low Outgassing Epoxy
Master Bond EP37-3FLFAO Low Outgassing Thermally Conductive Epoxy System
Master Bond EP38FLAO Two Component Epoxy
Master Bond EP30FL Low Viscosity, Flexibilized Two Component Epoxy
Tra-Con Tra-Bond K6 Ablative Thermal Epoxy Compound

PMASTB101 / 52258

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.