MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Crosspolimeri FRAGOM G/990 XA Flame Retardant Halogen Free Polyolefine
Categories: Polymer; Thermoplastic; Polyolefin

Material Notes: FRAGOM: is the trade-mark of our flame retardant halogen free polyolefine compounds.

FRAGOM G/990 XA: flame retardant crosslinkable EPR / HEPR / EPDM / POLYTHENE base compound having GOOD RESISTANCE TO OIL for insulation and sheathing. It is a conveniently grafted compound able to react in presence of moisture and of a catalyst. We normally suggest our catalyst type MAC/100 SCU. To use in solar cables sheathing (TUV) we suggest to add 10-11 % of catalyst MAC/500 UV REACTION BETW EEN GRAFTING AND CATALYST These two compounds, separately stored, must be mixed before starting extrusion in the ratio: GRAFTING/CATALYST 95/5

Certify: VDE0207-24 HM3, CEI 2011 M2-EM2, IEC 60092-359 SHF2, IEC 332-1, EN 50363 EI5, TUV

Information provided by Crosspolimeri S.P.A.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.45 g/ccASTM D792
Melt Flow 4.0 - 9.0 g/10 min
@Load 21.6 kg,
Temperature 190 °C
ASTM D1238
Storage Temperature 12.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 50ASTM D2240
Tensile Strength >= 10.0 MPaIEC 60811
 >= 7.50 MPa
@Temperature 100 °C,
Time 605000 sec
Ageing in IRM 902; IEC 60811
 >= 8.50 MPa
@Temperature 70.0 °C,
Time 605000 sec
Ageing in IRM 903 oil; IEC 60811
 >= 10.8 MPa
@Temperature 135 °C,
Time 864000 sec
Heat Ageing; IEC 60811
 >= 11.5 MPa
@Temperature 127 °C,
Time 144000 sec
air bomb; IEC 60811
Elongation at Break >= 125 %IEC 60811
 >= 50 %
@Temperature 190 °C,
Time 360000 sec
Heat Ageing; TUV/M21
 >= 76.25 %
@Temperature 70.0 °C,
Time 605000 sec
Ageing in IRM 903 oil; IEC 60811
 >= 103.75 %
@Temperature 127 °C,
Time 144000 sec
air bomb; IEC 60811
 >= 125 %
@Temperature 100 °C,
Time 605000 sec
Ageing in IRM 902; IEC 60811
 >= 131.25 %
@Temperature 135 °C,
Time 864000 sec
Heat Ageing; IEC 60811
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 3.9
@Frequency 50 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
Hot Ball Pressure Test 140 °C
@Time 14400 sec
<60%, (K=0,6)-penetratio; IEC 60811
Oxygen Index 35 %ASTM D2863
 
Processing PropertiesOriginal ValueComments
Zone 1 150 °C
Zone 2 160 °C
Zone 3 170 °C
Zone 4 175 °C
Die Temperature 205 °C
Head Temperature 180 °C
 
Descriptive Properties
Conductivity<10 µS/mmIEC 60754-2
Corrosivity of gases evolved>4,3 pHIEC 60754-2
Halogen Content< 0,3%IEC 60754-1
Hot Set Test0Residual Value, IEC 60811
 0.8250°C - 20 N/cm2, IEC 60811
Toxicity Index=2%CEI 20-37/4-0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCROS070 / 294154

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.