MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
SABIC CYCOLAC™ DL100LG ABS (Americas)
Categories: Polymer; Thermoplastic; ABS Polymer

Material Notes: CYCOLAC DL100LG is a low gloss, high heat, high impact ABS/PC blend with low emission

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.08 g/ccISO 1183
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cmSABIC method
Melt Flow 10 g/10 min
@Load 10.0 kg,
Temperature 220 °C
cm³/10 min; ISO 1133
 10 g/10 min
@Load 10.0 kg,
Temperature 220 °C
ASTM D1238
 12 g/10 min
@Load 5.00 kg,
Temperature 260 °C
cm³/10 min; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 80.0 MPaISO 2039-1
Tensile Strength at Break 36.0 MPa5 mm/min; ISO 527
 38.0 MPa50 mm/min; ASTM D638
 39.0 MPa50 mm/min; ISO 527
 40.0 MPa5 mm/min; ASTM D638
Tensile Strength, Yield 47.0 MPa5 mm/min; ASTM D638
 47.0 MPa5 mm/min; ISO 527
 51.0 MPa50 mm/min; ISO 527
 51.0 MPa50 mm/min; ASTM D638
Elongation at Break 12 %50 mm/min; ISO 527
 12 %50 mm/min; ASTM D638
 50 %5 mm/min; ISO 527
 85 %5 mm/min; ASTM D638
Elongation at Yield 4.0 %5 mm/min; ASTM D638
 4.0 %50 mm/min; ISO 527
 4.0 %50 mm/min; ASTM D638
 4.0 %5 mm/min; ISO 527
Tensile Modulus 2200 MPa1mm/min; ISO 527
 2240 MPa50 mm/min; ASTM D638
Flexural Yield Strength 74.0 MPa2 mm/min; ISO 178
Flexural Modulus 2200 MPa2 mm/min; ISO 178
Izod Impact, Notched 380 J/mASTM D256
 115 J/m
@Temperature -30.0 °C
ASTM D256
Izod Impact, Notched (ISO) 28.0 kJ/m²80*10*4; ISO 180/1A
 45.0 kJ/m²80*10*3; ISO 180/1A
 11.0 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
 19.0 kJ/m²
@Temperature -30.0 °C
80*10*3; ISO 180/1A
Charpy Impact, Notched 22.0 kJ/m²Edgew 80*10*3 sp=62mm; ISO 179/1eA
 11.0 kJ/m²
@Temperature -30.0 °C
Edgew 80*10*3 sp=62mm; ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 82.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 83.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 103 °CFlatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 84.0 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 85.0 °C
@Thickness 6.40 mm
unannealed; ASTM D648
Vicat Softening Point 105 °CRate B/50; ISO 306
 107 °CRate B/120; ISO 306
 118 °CRate A/50; ISO 306
 120 °CRate A/120; ISO 306
 
Processing PropertiesOriginal ValueComments
Processing Temperature 60.0 - 80.0 °CHopper Temperature
Nozzle Temperature 245 - 275 °CInjection Molding
Zone 1 230 - 260 °C
Zone 2 250 - 280 °C
Zone 3 250 - 280 °C
Melt Temperature 250 - 280 °C
Mold Temperature 40.0 - 80.0 °C
Drying Temperature 90.0 - 100 °CInjection Molding
Dry Time 2.00 - 4.00 hourInjection Molding
Moisture Content 0.10 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI10006 / 243473

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.