MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Röhm PLEXIGLAS® Softlight 7N df22 PMMA
Categories: Polymer; Thermoplastic; Acrylic (PMMA)

Material Notes: PLEXIGLAS® Softlight 7N df22, based on PLEXIGLAS® 7N, is characterized by diffuse scattering of light.

Typical properties of PLEXIGLAS® molding compound are

  • good flow
  • high mechanical strength, surface hardness and mar resistance.
Special properties of PLEXIGLAS® Softlight 7N df22 are
  • very good light diffusion combined with excellent light transmittance.
Application: Used for injection molding items for lighting engineering applications
  • very good light diffusion combined with excellent light transmittance.
Application: Used for injection molding items for lighting engineering applications

Information provided by Roehm America LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.19 g/ccISO 1183
Melt Flow 4.3 g/10 min
@Load 3.80 kg,
Temperature 230 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 65.0 MPa5 mm/min; ISO 527
Elongation at Break 2.5 %5 mm/min; ISO 527
Tensile Modulus 3.40 GPa1 mm/min; ISO 527
Charpy Impact Unnotched 17.0 kJ/m²ISO 179/1eU
Charpy Impact, Notched 1.80 kJ/m²ISO 179/1
 
Thermal PropertiesOriginal ValueComments
CTE, linear 6.30 µm/m-°C
@Temperature 0.000 - 50.0 °C
ISO 11359
Deflection Temperature at 0.46 MPa (66 psi) 101 °CISO 75
Deflection Temperature at 1.8 MPa (264 psi) 97.0 °CISO 75
Vicat Softening Point 105 °CB / 50; ISO 306
Glass Transition Temp, Tg 108 °CISO 11357
Glow Wire Ignition Temperature 700 °CIEC 60695-2
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 86 %ISO 13468-2
 
Processing PropertiesOriginal ValueComments
Die Temperature 220 - 260 °CExtrusion
Melt Temperature 220 - 260 °C
Drying Temperature <= 95.0 °CPredrying
Dry Time 2.00 - 3.00 hourPredrying, Desiccant-Type Drier
 
Descriptive Properties
Half-Value Angle12.6°DIN 5036

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PROHM9363 / 319980

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.