Cas No. 77-58-7 GOYENCHEM-DBTL is an important PU catalyst for catalyzing the reaction of carboxyl groups with isocyanates. It is also widely used in PU related products such as adhesives, coatings, sealants, elastomers and so on. Effectively promote the chain growth, speed up the curing process. Advantages: - Excellent weather resistance
- Outstanding heat resistance
- Great transparency
- Odorless
- Superb catalyst reaction efficiency
Applications : - PU catalyst
- PU resin reaction synthesis catalyst
- PU foam catalyst
- Polyurethane series related products such as adhesives, coatings, sealants, elastomers
- Soft and rigid foam
Information provided by Go Yen Chemical |