MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Chemours Zonyl™ MP 1200 PTFE Additive
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes: Zonyl™ MP 1200 fluoroadditive is a white, free-flowing, PTFE powder designed for use as an additive in other materials or as a dry lubricant. It can be used at temperatures from –190 °C to 250 °C (–310 °F to 480 °F) and is inert to nearly all industrial chemicals and solvents. It is a good electrical insulator, does not absorb water, and is highly resistant to weathering. Applications: Zonyl™ MP 1200 is used as an additive (at approximately 1–3% by weight) in the preparation of offset, gravure, and flexographic printing inks. It improves certain properties, such as rub and slip resistance. It is used in combination with polyethylene waxes to obtain the desired degree of property modification. Due to its small particle size and narrow particle size distribution, Zonyl™ MP 1200 has been found useful in a variety of coating systems. Typical loadings of 5–20% by weight are used in plastics and elastomers. Provides improvements in corrosion inhibition, Reduces wettability, Reduces “blocking” in inks, Improves gloss and surface smoothness.

Information provided by Chemours.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.450 g/ccASTM D4894
Specific Surface Area 1.5 - 3.0 m²/gASTM D4567
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 250 °C
Minimum Service Temperature, Air -190 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDU8854 / 268781

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.