Styrene-Butadiene Rubber can be used in tire industry-for production of tire thread and other parts for tires. In rubber technical industry- for production of wide assortment of rubber technical articles. In shoes industry, for production of white and colored rubber footwear.Information provided by Shanghai Potomer International Trade Co., Ltd |