NORYL GTX™ 8110P resin is a 10% glass reinforced alloy of Polyphenylene Ether (PPE) + Polyamide (PA). This extrudable grade has excellent chemical resistance, and high heat resistance. NORYL GTX8110P resin is anodizable, has low thermal conductivity, and is an excellent candidate for extruded thermal break applications. Features: Extrusion Grade,Thermally Conductive Information provided by SABIC |