MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Copper Alloy, UNS C71950,
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Temper: Spinodal Hardened-Low Strength (ATLS)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.318 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 170 - 250
@Load 3000 kg
Tensile Strength 87.0 ksiTypical
 80.0 - 119 ksi
Tensile Strength, Yield 61.0 ksi0.2% Offset, Typical
 51.0 - 105 ksi0.2% Offset
Elongation at Break 20 - 27 %
Tensile Modulus 20200 ksi
Modulus of Rigidity 7820 ksi
Poissons Ratio 0.30
Shear Strength 39.0 ksi
Impact Test 81.13 ft-lb
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000430 ohm-cm4% IACS
Magnetic Permeability 1.01
 
Thermal PropertiesOriginal ValueComments
CTE, linear 10.0 µin/in-°F
@Temperature 20.0 - 300 °C
Thermal Conductivity 13.3 BTU-in/hr-ft²-°F
Melting Point 2120 - 2204 °F
Solidus 2120 °F
Liquidus 2204 °F
 
Component Elements PropertiesOriginal ValueComments
Bismuth, Bi <= 0.0010 %
Boron, B <= 0.0010 %
Carbon, C <= 0.020 %
Chromium, Cr 1.6 - 2.0 %
Cobalt, Co <= 0.050 %
Copper, Cu 63.2 - 68.1 %As Balance
Iron, Fe 0.50 - 1.0 %
Lead, Pb <= 0.0050 %
Manganese, Mn 0.50 - 1.0 %
Nickel, Ni 29 - 32 %
Phosphorus, P <= 0.0050 %
Silicon, Si 0.20 - 0.40 %
Sulfur, S <= 0.0050 %
Titanium, Ti 0.030 - 0.15 %
Zirconium, Zr 0.050 - 0.15 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

MC71950x1 / 292456

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.