MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Corning PHOTOGRAY THIN & DARK™ Wide range photochromic glass for thin lenses
Categories: Ceramic; Glass; Optical

Material Notes: Application : Ophthalmic lenses : Single vision, G&P progressive addition

Information provided by Corning Incorporated.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.38 g/cc
 
Thermal PropertiesOriginal ValueComments
CTE, linear 6.22 µm/m-°C
Softening Point 634 °C
Annealing Point 493 °C
Strain Point 634 °C
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.52021
@Wavelength 656.3 nm
Line: C; Hydrogen
 1.52063
@Wavelength 643.8 nm
Line: C'; Cadmium
 1.523
@Wavelength 587.6 nm
Line: d; Helium
 1.52518
@Wavelength 546.1 nm
Line: e; Mercury
 1.52938
@Wavelength 486.1 nm
Line: F; Hydrogen
 1.52989
@Wavelength 480 nm
Line: F'; Cadmium
Abbe Number 56.7ve
 57vd
Transmission, Visible 14 %
@Wavelength 380 - 780 nm,
Thickness 2.00 mm
Luminous, Darkened
 14 %
@Wavelength 380 - 500 nm,
Thickness 2.00 mm
Blue light transmission factor, Darkened
 86.5 %
@Wavelength 380 - 500 nm,
Thickness 2.00 mm
Blue light transmission factor, Faded
 91 %
@Wavelength 380 - 780 nm,
Thickness 2.00 mm
Luminous, Faded
UV Transmittance <= 0.10 %
@Thickness 2.00 mm
Solar UV-B transmission factor, Faded
 <= 0.10 %
@Thickness 2.00 mm
Solar UV-B transmission factor, Darkened
 1.0 %
@Thickness 2.00 mm
Solar UV-A transmission factor, Darkened
 9.5 %
@Thickness 2.00 mm
Solar UV-A transmission factor, Faded
 <= 0.10 %
@Wavelength 280 - 315 nm,
Thickness 2.00 mm
t(max), Faded
 <= 0.10 %
@Wavelength 280 - 315 nm,
Thickness 2.00 mm
t(max), Darkened
 <= 0.10 %
@Wavelength 280 - 315 nm,
Thickness 2.00 mm
t(avg), Faded
 <= 0.10 %
@Wavelength 280 - 315 nm,
Thickness 2.00 mm
t(avg), Darkened
 1.0 %
@Wavelength 315 - 350 nm,
Thickness 2.00 mm
t(max), Darkened
 1.5 %
@Wavelength 380 - 500 nm,
Thickness 2.00 mm
t(moy), Darkened
 10 %
@Wavelength 315 - 350 nm,
Thickness 2.00 mm
t(max), Faded
 13 %
@Wavelength 380 - 500 nm,
Thickness 2.00 mm
t(moy), Faded
 
Descriptive Properties
ColorClear to Dark gray

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

CCORN921 / 233332

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.