Greenflex ML 21 is an ethylene vinyl acetate copolymer (EVA) for injection molding, when a good ESCR is required. Greenflex ML 21 contains additive waxes to obtain high production speed. Main Applications: Greenflex ML 21 is suitable for the production of flexible items. Information provided by Polimeri Europa. Versalis is the Eni subsidiary containing the plastics and rubber businesses. |