MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Tra-Con Tra-Bond CA20 Coil-Fix Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Filled/Reinforced Thermoset

Material Notes: TRA-BOND CA-20 is a thixotropic epoxy adhesive system specially formulated for shorted turns, damaged end wire extensions, or other coil repair applications where a high-fill, non-sag adhesive is required. It is dark-red to brown in color to blend with many commonly used insulating varnishes, and it provides a combination of high dielectric isolation coupled with good mechanical strength. Solvent-free TRA-BOND CA-20 is readily mixed, handled, used and cured at room temperature and develops strong bonds to most materials, including metals, glass, ceramics, and many other coil coatings and insulators. When fully cured, this epoxy adhesive provides excellent resistance to galvanic action, petroleum lubricants and solvents, salts, mild acids and alkalis, other organic and inorganic compounds, and weather.

Information provided by Tra-Con Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.24 g/cc1.24 g/ccMixed
Viscosity 27000 cP
@Temperature 25.0 °C
27000 cP
@Temperature 77.0 °F
After mixing
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 9090
Izod Impact, Notched 0.267 J/cm0.500 ft-lb/in
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 6.00e+13 ohm-cm6.00e+13 ohm-cm
 1.00e+10 ohm-cm
@Temperature 100 °C
1.00e+10 ohm-cm
@Temperature 212 °F
Dielectric Constant 4.2
@Frequency 1000 Hz
4.2
@Frequency 1000 Hz
Dielectric Strength 15.7 kV/mm400 kV/in
 
Thermal PropertiesMetricEnglishComments
CTE, linear 55.0 µm/m-°C
@Temperature 20.0 °C
30.6 µin/in-°F
@Temperature 68.0 °F
Maximum Service Temperature, Air 115 °C239 °F
Minimum Service Temperature, Air -60.0 °C-76.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  240 min
@Temperature 65.0 °C
4.00 hour
@Temperature 149 °F
 1440 min
@Temperature 25.0 °C
24.0 hour
@Temperature 77.0 °F
Pot Life 30 min30 min
 
Descriptive Properties
Color Dark Red
Mix Ratio, parts by weight100/22Resin/Hardener

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M Scotchcast™ 265 Electrical Epoxy Powder Resin
3M Scotchcast™ 5555 22G Electrical Insulating Epoxy Resin
Dymax 928 Coil Terminating, Tamper proofing and Structural Electronic Bonder
Dymax 9-20524 Voil Coil Assembly Disk Drive Adhesive
Dymax 9-20512 Voil Coil Assembly Disk Drive Adhesive

PTRAC219 / 71147

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.