MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Morgan Advanced Ceramics Thermatex 850 Paper Thermal Ceramic
Categories: Ceramic; Oxide

Material Notes: Thermatex 850 Paper is one of a range of Thermal Ceramics refractory fiber papers, and has been developed specifically as an asbestos paper replacement. It is a soft, flexible, clean paper that is pleasant to handle. Standard roll widths include 500mm, 610mm, 1000mm and 1220mm. Alternatively, Thermatex 850 Paper can be supplied die cut to regular or intricate flat shapes to suit specific application requirements. Thermatex 850 Paper application areas include the primary aluminium industry, non-ferrous foundries and the general domestic appliance market. Additionally, it is ideal for low-pressure seals and gaskets for temperatures up to 850°C.

Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramics
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.180 - 0.200 g/cc0.00650 - 0.00723 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 0.00100 MPa0.145 psilongitudinal
 0.500 MPa72.5 psitransverse
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity  0.0400 W/m-K
@Temperature 100 °C
0.278 BTU-in/hr-ft²-°F
@Temperature 212 °F
 0.0840 W/m-K
@Temperature 300 °C
0.583 BTU-in/hr-ft²-°F
@Temperature 572 °F
 0.130 W/m-K
@Temperature 500 °C
0.902 BTU-in/hr-ft²-°F
@Temperature 932 °F
Melting Point >= 1000 °C>= 1830 °F
 
Component Elements PropertiesMetricEnglishComments
Al2O3 21 %21 %
CaO+MgO 25 %25 %
Fe2O3 6.0 %6.0 %
Loss on Ignition(%) 4.5 - 9.0 %4.5 - 9.0 %
Other 8.0 %8.0 %
SiO2 40 %40 %
 
Descriptive Properties
Acoustic Absorption Coefficient0.05at 100Hz
 0.21at 2000Hz
 0.4at 4000 Hz
Classification Temperature (°C)850
Colorlight green
Fiber Diameter0.5 µm
Fiber Index<15 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Electrolytic Copper Tough Pitch, 50% hard-drawn rod
3M Interam™ E-5A-4 Endothermic Mat

CMORF7099 / 203397

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.