MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Lubrizol Advanced Materials Pearlstick® 45-40/08 Polycaprolactone based TPU
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Pearlstick® 45-40/08 is an elastic, linear, aromatic polyurethane, supplied in form of white spherical granules with a very high crystallization rate and a medium thermoplasticity level.

Solubility: Pearlstick® 45-40/08 is soluble in Acetone, Methyl Ethyl Ketone (MEK), Cyclohexanone, Dimethyl formamide, (DMF), Tetrahydrofurane (THF). Diluting solvents such as Toluene and Ethyl Acetate can be added. The solvents and diluents should be water-free (max. 0.1%), so as to avoid subsequent side reactions during crosslinking with isocyanate. Pearlstick® 45-40/08 should be dissolved in closed tanks and the use of a variable speed agitator is advisable. The final viscosity figures can vary, depending on the stirring process and on the solvent/diluents ratios.

Applications: Pearlstick® 45-40/08 is used for the production of adhesives for bonding plasticized PVC to plasticized PVC or other materials such as leather, textiles, etc. Pearlstick® 45-40/08 enables the production of adhesives for spray application for the automotive and other industrial uses. The addition of a polyfunctional isocyanate improves the heat-resistance and the strength of the joints.

Information provided by Merquinsa

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.19 g/cc0.0430 lb/in³ISO 2781
Brookfield Viscosity 650 - 950 cP650 - 950 cPBrookfield RVF sp 2, 20 rpm, Solution 15% MEK (MQSA Nº 55 A); MQSA 40A
 
Processing PropertiesMetricEnglishComments
Processing Temperature 45.0 °C113 °FMin. Activation Temp; EN 12961
 
Descriptive Properties
Crystallization Rate (MQSA n° 12 A)VERY HIGH
Hydrolysis resistanceGoodMQSA 34B
Hydroxyl number0.1%MQSA 47A
Solubility - Acetone / Ethyl Acetate30:70
Solubility - Acetone / Toluene40:60
Solubility - MEK / Toluene60:40
Solubility - MEK/ Ethyl Acetate40:60
Thermoplasticity Range (MQSA n° 58)MEDIUM

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polycarbonate/Thermoplastic Polyurethane Blend
Lubrizol Advanced Materials Pearlthane® 11T85 Polycaprolactone Copolyester based TPU
Lubrizol Advanced Materials Pearlstick® 45-40/27 Polycaprolactone based TPU
Lubrizol Advanced Materials Pearlstick® 45-40/19 Polycaprolactone based TPU
Lubrizol Advanced Materials Pearlstick® 45-40/15 Polycaprolactone based TPU

PMER72 / 52871

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.