MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

BASF Ultraform® N2644 Z9 POM + PUR
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Unreinforced

Material Notes: Description: Elastomer modified injection molding grade for applications requiring low modulus. Good acoustic damping.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.650 - 0.850 g/cc0.0235 - 0.0307 lb/in³
Density 1.27 g/cc0.0459 lb/in³ISO 1183
Water Absorption 0.50 %0.50 %ISO 62
Moisture Absorption at Equilibrium 0.20 %0.20 %ISO 62
Linear Mold Shrinkage, Flow 0.012 cm/cm0.012 in/inISO 2577
Linear Mold Shrinkage, Transverse 0.0148 cm/cm0.0148 in/inISO 2577
Melt Flow 15.24 g/10 min
@Load 2.16 kg,
Temperature 190 °C
15.24 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 30.0 MPa
@Load 13.5 kg,
Time 30.0 sec
4350 psi
@Load 29.7 lb,
Time 0.00833 hour
ISO 2039-1
Tensile Strength, Yield 22.0 MPa3190 psi50 mm/min; ISO 527-1/-2
Elongation at Break 50 %50 %50 mm/min, Nominal; ISO 527-1/-2
Elongation at Yield 25 %25 %50 mm/min; ISO 527-1/-2
Tensile Modulus 0.700 GPa102 ksiISO 527-1/-2
Charpy Impact Unnotched  NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179/1eU
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched  0.500 J/cm²
@Temperature -30.0 °C
2.38 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 0.850 J/cm²
@Temperature 23.0 °C
4.04 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+11 ohm-cm1.00e+11 ohm-cmIEC 60093
Surface Resistance 1.00e+12 ohm1.00e+12 ohmIEC 60093
Dielectric Constant 5.0
@Frequency 1e+6 Hz
5.0
@Frequency 1e+6 Hz
IEC 60250
Dissipation Factor 0.026
@Frequency 1e+6 Hz
0.026
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 V600 VTest Solution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 140 µm/m-°C
@Temperature 23.0 - 55.0 °C
77.8 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1/-2
Melting Point 164 °C327 °FISO 11357-1/-3
Maximum Service Temperature, Air 100 °C212 °F
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °C131 °FISO 75-1/-2
Decomposition Temperature >= 240 °C>= 464 °F
Flammability, UL94 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
Ignition Temperature 320 - 340 °C608 - 644 °FASTM D1929
 
Processing PropertiesMetricEnglishComments
Processing Temperature 200 °C392 °FHopper Throat
Zone 1 200 °C392 °FFeed zone
Zone 2 200 °C392 °FCompression
Zone 3 200 °C392 °FMetering-zone
Zone 4 200 °C392 °FNozzle
Melt Temperature 200 °C392 °FOptimal
 190 - 215 °C374 - 419 °FInjection molding
Mold Temperature 60.0 °C140 °FOptimal
 60.0 - 80.0 °C140 - 176 °FInjection molding
Drying Temperature 100 °C212 °F
Dry Time 3 hour3 hour
 
Descriptive Properties
Commercial StatusEurope
Peripheral Screw Speed<0.3 m/s
Primary Processing TechniqueInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultraform® N2640 Z2 POM + PUR
Chase Plastics CP Pryme® AH120 Acetal Copolymer, 20% Glass Fiber Reinforced
Delrin Delrin® 100AF POM-PTFE20
3M Scotch-Weld™ EZ250150 Polyurethane Reactive (PUR) Easy 250 Wood Adhesive
3M Scotch-Weld™ EZ250015 Polyurethane Reactive (PUR) Easy 250 Wood Adhesive

PBASG0164 / 131797

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.