Product Description: Grilamid L 25 H FWA black 9225 is a highviscosity, unreinforced and heat stabilized Polyamide 12 (PA12). Grilamid L 25 H FWA black 9225 is designed for technical injection moulded components, and is in particular suitable for parts with medium or high wall thicknesses. The maximum thickness can largely exceed 15 mm.- high impact strength
- high elongation
- very low moisture absorption
- good chemical resistance
- high melt viscosity
- easy processing
- low density
Application examples: The particular stabilisation package of Grilamid L 25 H FWA black 9225 allows the use in direct contact with potable water and foodstuff.Information provided by EMS Grivory |