MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

AISI 1039 Steel, cold drawn, 19-32 mm (0.75-1.25 in) round
Categories: Metal; Ferrous Metal; Carbon Steel; AISI 1000 Series Steel; Medium Carbon Steel

Key Words: B. S. 120 M 26 (UK), B. S. 150 M 36 (UK), B. S. CDS 105, DIN 1.1157, AFNOR 35 M 5, SAE J403, SAE J412, SAE J414, UNS G10390, ASTM A29, ASTM A510, ASTM A546, ASTM A576
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.845 g/cc0.2834 lb/in³Chemical composition of 0.435% C, 0.69% Mn, 0.20% Si, annealed at 860°C (1580°F).
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 179179
Hardness, Knoop 204204Converted from Brinell Hardness
Hardness, Vickers 187187Converted from Brinell Hardness
Tensile Strength, Ultimate 605 MPa87700 psi
Tensile Strength, Yield 510 MPa74000 psi
Elongation at Break 12 %12 %
Reduction of Area 35 %35 %
Bulk Modulus 160 GPa23200 ksiTypical for steel
Shear Modulus 80.0 GPa11600 ksiTypical for steel
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity  0.0000171 ohm-cm
@Temperature 20.0 °C
0.0000171 ohm-cm
@Temperature 68.0 °F
 0.0000221 ohm-cm
@Temperature 100 °C
0.0000221 ohm-cm
@Temperature 212 °F
 0.0000296 ohm-cm
@Temperature 200 °C
0.0000296 ohm-cm
@Temperature 392 °F
 0.0000493 ohm-cm
@Temperature 400 °C
0.0000493 ohm-cm
@Temperature 752 °F
 0.0000763 ohm-cm
@Temperature 600 °C
0.0000763 ohm-cm
@Temperature 1110 °F
 0.0000932 ohm-cm
@Temperature 700 °C
0.0000932 ohm-cm
@Temperature 1290 °F
 0.0001111 ohm-cm
@Temperature 800 °C
0.0001111 ohm-cm
@Temperature 1470 °F
 0.0001149 ohm-cm
@Temperature 900 °C
0.0001149 ohm-cm
@Temperature 1650 °F
 0.0001179 ohm-cm
@Temperature 1000 °C
0.0001179 ohm-cm
@Temperature 1830 °F
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 0.486 J/g-°C
@Temperature >=100 °C
0.116 BTU/lb-°F
@Temperature >=212 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.36 - 0.44 %0.36 - 0.44 %
Iron, Fe 98.47 - 98.94 %98.47 - 98.94 %As remainder
Manganese, Mn 0.70 - 1.0 %0.70 - 1.0 %
Phosphorus, P <= 0.040 %<= 0.040 %
Sulfur, S <= 0.050 %<= 0.050 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI 1038 Steel, cold drawn, 19-32 mm (0.75-1.25 in) round
AISI 1039 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round
AISI 1045 Steel, cold drawn, 19-32 mm (0.75-1.25 in) round
AISI 1038 Steel, hot rolled round, 19-32 mm (0.75-1.25 in)
AISI 1040 Steel, as cold drawn, 16-22 mm (0.625-0.875 in) round

M1039A / 6932

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.