MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Crosspolimeri EFRHATAN 95 A4 05 Polyurethane-Polyether Flame Retardant
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyether Grade

Material Notes: Efrhatan: is the trade-mark of our modified polyurethane-polyether flame retardant halogen free. The type 95 A4 05 maintains matt surface.

Efrhatan 95 A4 05: is a thermoplastic elastomeric polyurethane HFFR compound polyether basis. This compound offer outstanding chemical and hydrolysis resistance. The material exhibit excellent physical-mechanical performances resulting in tubes and sheathings with optimal kink resistance, strength characteristics and flame retardance. Good processability and excellent extrusion stability. Material to use on the production of cables for electronic devices connection and technical sheathing. Principal cables construction are H07BQ-F,H05BQ-F.

Certify: HD 221,VDE 0282-10,UL 1581 VW-1,IEC 60332-3

Information provided by Crosspolimeri S.P.A.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.29 g/cc1.29 g/ccISO 1183
Storage Temperature 12.0 °C53.6 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9595ISO 868
Tensile Strength 15.0 MPa2180 psiISO 527
 18.0 MPa
@Temperature 120 °C,
Time 605000 sec
2610 psi
@Temperature 248 °F,
Time 168 hour
Heat Ageing; UL 1581
 18.0 MPa
@Temperature 100 °C,
Time 605000 sec
2610 psi
@Temperature 212 °F,
Time 168 hour
Oil resistance, ASTM II; UL 1581
Elongation at Break 350 %350 %ISO 527
 455 %
@Temperature 120 °C,
Time 605000 sec
455 %
@Temperature 248 °F,
Time 168 hour
Heat Ageing; UL 1581
 455 %
@Temperature 100 °C,
Time 605000 sec
455 %
@Temperature 212 °F,
Time 168 hour
Oil resistance, ASTM II; UL 1581
Tear Strength >= 60.0 kN/m>= 342 pliambient; DIN 53515
Abrasion >= 40>= 40[mm³]; DIN 53516
 
Thermal PropertiesMetricEnglishComments
Flammability, UL94 V-0V-0
Oxygen Index 27 %27 %ASTM D2863
 
Processing PropertiesMetricEnglishComments
Zone 1 170 °C338 °F
Zone 2 180 °C356 °F
Zone 3 180 °C356 °F
Zone 4 200 °C392 °F
Die Temperature 190 °C374 °F
Head Temperature 200 °C392 °F
Dry Time  3.00 hour
@Temperature 90.0 °C
3.00 hour
@Temperature 194 °F
 6.00 hour
@Temperature 90.0 °C
6.00 hour
@Temperature 194 °F
 
Descriptive Properties
Cold Flex-40°CISO 458
Saponification Resistance<200 Mg KOH/gHD 22.10S1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCROS036 / 294120

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.