MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Titanium Grade 4, Annealed
Categories: Metal; Nonferrous Metal; Titanium Alloy; Unalloyed/Modified Titanium

Material Notes: Information provided by Allvac and the references.

Applications: Airframe components, cryogenic vessels, heat exchangers, CPI equipment, condenser tubing, pickling baskets. Sample was annealed 2 hr at 700°C.

Forms typically available: billet, bar, plate, sheet, strip, rod, wire, extrusions, tubing.

Titanium Grades 1,2,3,4,7,11,and 12 are all considered unalloyed and have similar mechanical properties.

Key Words: ASTM Grade 4: UNS R50700, CP titanium, C.P. titanium alloy
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 4.51 g/cc0.163 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 265265
Hardness, Knoop 296296Estimated from Brinell.
Hardness, Rockwell B 104104
Hardness, Rockwell C 2323Estimated from Brinell.
Hardness, Vickers 280280Estimated from Brinell.
Tensile Strength 310 MPa
@Temperature 316 °C
45000 psi
@Temperature 601 °F
Tensile Strength, Ultimate 660 MPa95700 psi
Tensile Strength, Yield 590 MPa85600 psi
Elongation at Break 20 %20 %
Tensile Modulus 105 GPa15200 ksiUnspecified heat treatment
Modulus of Rigidity 38.6 GPa5600 ksi
Compressive Modulus 110 GPa16000 ksiunspecified heat treatment
Notched Tensile Strength 900 MPa131000 psiKt (stress concentration factor) = 3.0
Poissons Ratio 0.340.34
Shear Modulus 39.0 GPa5660 ksi
Bend Radius, Minimum 3.0 t
@Thickness >=1.80 mm
3.0 t
@Thickness >=0.0709 in
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000600 ohm-cm0.0000600 ohm-cm
 0.0000950 ohm-cm
@Temperature 250 °C
0.0000950 ohm-cm
@Temperature 482 °F
 0.000130 ohm-cm
@Temperature 500 °C
0.000130 ohm-cm
@Temperature 932 °F
 0.000155 ohm-cm
@Temperature 750 °C
0.000155 ohm-cm
@Temperature 1380 °F
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 325 J/g140 BTU/lbHigh Purity Ti.
CTE, linear  8.60 µm/m-°C
@Temperature 20.0 - 93.0 °C
4.78 µin/in-°F
@Temperature 68.0 - 199 °F
 9.20 µm/m-°C
@Temperature 200 °C
5.11 µin/in-°F
@Temperature 392 °F
 19.9 µm/m-°C
@Temperature 20.0 °C
11.1 µin/in-°F
@Temperature 68.0 °F
perpendicular
Specific Heat Capacity 0.540 J/g-°C0.129 BTU/lb-°F
 0.560 J/g-°C
@Temperature 200 °C
0.134 BTU/lb-°F
@Temperature 392 °F
 0.620 J/g-°C
@Temperature 400 °C
0.148 BTU/lb-°F
@Temperature 752 °F
 0.690 J/g-°C
@Temperature 600 °C
0.165 BTU/lb-°F
@Temperature 1110 °F
Thermal Conductivity 16.9 W/m-K117 BTU-in/hr-ft²-°F
 16.8 W/m-K
@Temperature 200 °C
117 BTU-in/hr-ft²-°F
@Temperature 392 °F
 17.1 W/m-K
@Temperature 400 °C
119 BTU-in/hr-ft²-°F
@Temperature 752 °F
 18.8 W/m-K
@Temperature 600 °C
130 BTU-in/hr-ft²-°F
@Temperature 1110 °F
 20.2 W/m-K
@Temperature 800 °C
140 BTU-in/hr-ft²-°F
@Temperature 1470 °F
Melting Point <= 1660 °C<= 3020 °F
Liquidus 1660 °C3020 °F
Beta Transus 950 °C1740 °F
 
Optical PropertiesMetricEnglishComments
Emissivity (0-1) 0.30
@Temperature 710 °C
0.30
@Temperature 1310 °F
High purity Ti
Reflection Coefficient, Visible (0-1) 0.560.56High purity Ti; visible light.
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.10 %<= 0.10 %
Hydrogen, H <= 0.015 %<= 0.015 %
Iron, Fe <= 0.50 %<= 0.50 %
Nitrogen, N <= 0.050 %<= 0.050 %
Other, each <= 0.050 %<= 0.050 %
Other, total <= 0.30 %<= 0.30 %
Oxygen, O <= 0.40 %<= 0.40 %
Titanium, Ti 99 %99 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Titanium Grade 4
Titanium Grade 2, Annealed
Titanium Grade 3, Annealed
Titanium Ti-6Al-4V (Grade 5), Annealed
Titanium Grade 3

MTU041 / 14264

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.