MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Plastics Group Polifil® C-30 30% Calcium Carbonate-Reinforced Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 30% Calcium Carbonate (CaCO3) Filler

Material Notes: Polifil® C series compounds are homopolymer polypropylene resins reinforced with fine particle size calcium carbonate. They combine high impact with stiffness, heat aging, good colorability, resistance to environmental stress-cracking, good surface and low mold shrinkage.

Applications:

  • Appliances
  • Electrical components
  • Housewares
  • Toys
  • Automotive
  • Utility products

Standard processing techniques are applicable.

Information provided by The Plastics Group.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.15 g/cc0.0415 lb/in³ASTM D792
Filler Content 30 %30 %ASTM D2584
Linear Mold Shrinkage 0.0090 cm/cm
@Thickness 1.59 mm
0.0090 in/in
@Thickness 0.0625 in
ASTM D955
Melt Flow 8.0 - 12 g/10 min8.0 - 12 g/10 min230/2.16; May be specified; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 9898ASTM D785
Tensile Strength at Break 25.5 MPa3700 psiASTM D638
Flexural Modulus 2.07 GPa300 ksiTangent; ASTM D790
Izod Impact, Notched 0.464 J/cm0.870 ft-lb/inAt 73°F; ASTM D256
Izod Impact, Unnotched 8.54 J/cm16.0 ft-lb/inAt 73°F; ASTM D256
Gardner Impact 1.24 J0.917 ft-lbASTM D3029
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 104 °C220 °FASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polypropylene with 30% Calcium Carbonate (CaCO3) Filler
Entec Hypro™ F PPH-CC30 Natural Homopolymer Polypropylene, 30% Calcium Carbonate Filled
Entec Hypro™ F PPC-CC30 Natural Copolymer Polypropylene, 30% Calcium Carbonate Filled
Albis Plastics Polypropylene PP 14A12 KR 30 , 30% Calcium Carbonate (CaCO3)
Albis Plastics Polypropylene PP 14A12 CaCO3 30 , 30% Calcium Carbonate (CaCO3)

PPOLI012 / 56916

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.