MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chi Mei Kibiton® PB-5925 SBC  (discontinued **)
Categories: Polymer; Thermoplastic; Styrene-Butadiene; Styrene-Butadiene Copolymer, SBC

Material Notes: Transparency, high stiffness, injection grade

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.01 g/cc0.0365 lb/in³ISO 1183
Melt Flow 11 g/10 min
@Load 5.00 kg,
Temperature 200 °C
11 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7272
Tensile Strength at Break 19.0 MPa2760 psi50 mm/min, 4 mm; ISO 527
Tensile Strength, Yield 32.0 MPa4640 psi50 mm/min, 4 mm; ISO 527
Elongation at Break 43 %43 %50 mm/min, 4mm; ISO 527
Elongation at Yield 2.0 %2.0 %50 mm/min, 4 mm; ISO 527
Flexural Strength 43.0 MPa6240 psi2 mm/min, 4 mm; ISO 178
Flexural Modulus 1.80 GPa261 ksi2 mm/min, 4 mm; ISO 178
Izod Impact, Notched 0.246 J/cm
@Thickness 6.35 mm,
Temperature 23.0 °C
0.460 ft-lb/in
@Thickness 0.250 in,
Temperature 73.4 °F
ASTM D256
Izod Impact, Notched (ISO) 2.30 kJ/m²1.09 ft-lb/in²ISO 180/1A
Charpy Impact Unnotched 1.30 J/cm²6.19 ft-lb/in²ISO 179
Charpy Impact, Notched 0.260 J/cm²1.24 ft-lb/in²ISO 179
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 71.0 °C160 °Funannealed; ISO 75
 83.0 °C181 °Fannealed; ISO 75
Vicat Softening Point  73.0 °C
@Load 5.00 kg
163 °F
@Load 11.0 lb
120°C/hr; ISO 306
 75.0 °C
@Load 5.00 kg
167 °F
@Load 11.0 lb
50°C/hr; ISO 306
 92.0 °C
@Load 1.00 kg
198 °F
@Load 2.20 lb
120°C/hr; ISO 306
 95.0 °C
@Load 1.00 kg
203 °F
@Load 2.20 lb
50°C/hr; ISO 306
 
Optical PropertiesMetricEnglishComments
Haze 2.5 %
@Thickness 3.17 mm
2.5 %
@Thickness 0.125 in
ASTM D1003

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chi Mei Kibiton® PB-511 SBC
Kraton® D1192 A (SBS) Liner Block Copolymer
Chi Mei Kibiton® PB-5502 Styrene-Butadiene Copolymer
Chi Mei Kibiton® PB-5903 SBC
Chi Mei Kibiton® PB-585R SBC

PCHI981 / 109469

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.