MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemours Krytox™ 143AB PFPE Aerospace Grade Fluorinated Oil
Categories: Fluid; Lubricant; Perfluoropolyether (PFPE)

Material Notes: Many grades and special formulations of Krytox™ oils and greases offer superior performance characteristics and certifications for aerospace applications. They operate effectively in high vacuum and extreme temperatures, and are able to endure exposure to fuels, oxidizers, and radiation.

Features:

  • Unaffected lubricity and viscosity within a wide temperature range
  • Stable physical properties over time, including radiation resistance
  • Virtually unaffected by harsh environments and caustic chemicals
  • Resistant to vapor loss in a vacuum (e.g., during high-altitude orbit or deep space flight)
  • Long wear and low-energy consumption due to excellent friction-reducing characteristics
  • Compatible for use with most metals, elastomers, plastics, paints, and finishes,
  • Nontoxic, nonflammable, inert, and non-evaporative.

Information provided by Chemours Krytox

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density  1.75 g/cc
@Temperature 100 °C
0.0632 lb/in³
@Temperature 212 °F
oil
 1.93 g/cc
@Temperature 0.000 °C
0.0697 lb/in³
@Temperature 32.0 °F
oil
Volatiles  1.9 %
@Treatment Temp. 149 °C,
Time 79200 sec
1.9 %
@Treatment Temp. 300 °F,
Time 22.0 hour
wt% loss; ASTM D2595
 17.3 %
@Treatment Temp. 204 °C,
Time 79200 sec
17.3 %
@Treatment Temp. 399 °F,
Time 22.0 hour
wt% loss; ASTM D2595
 76.2 %
@Treatment Temp. 260 °C,
Time 79200 sec
76.2 %
@Treatment Temp. 500 °F,
Time 22.0 hour
wt% loss; ASTM D2595
Viscosity Measurement 113113Viscosity Index; ASTM D2270
Viscosity Measure  2.1 cSt
@Temperature 204 °C
2.1 cSt
@Temperature 399 °F
ASTM D445
 10.2 cSt
@Temperature 100 °C
10.2 cSt
@Temperature 212 °F
ASTM D445
 10.5 cSt
@Temperature 99.0 °C
10.5 cSt
@Temperature 210 °F
ASTM D445
 78 cSt
@Temperature 40.0 °C
78 cSt
@Temperature 104 °F
ASTM D445
 86 cSt
@Temperature 38.0 °C
86 cSt
@Temperature 100 °F
ASTM D445
 240 cSt
@Temperature 20.0 °C
240 cSt
@Temperature 68.0 °F
ASTM D445
 1070 cSt
@Temperature 0.000 °C
1070 cSt
@Temperature 32.0 °F
ASTM D445
 44620 cSt
@Temperature -32.0 °C
44620 cSt
@Temperature -25.6 °F
ASTM D445
Molecular Weight 3800 g/mol3800 g/molNMR
Vapor Pressure  6.67e-9 bar
@Temperature 38.0 °C
0.00000500 torr
@Temperature 100 °F
Knudsen
 0.0000800 bar
@Temperature 260 °C
0.0600 torr
@Temperature 500 °F
Knudsen
 
Thermal PropertiesMetricEnglishComments
Distillation Temperature 215 - 290 °C
@Pressure 0.0000530 MPa
419 - 554 °F
@Pressure 0.00769 psi
ASTM D1160
Maximum Service Temperature, Air 232 °C450 °F
Minimum Service Temperature, Air -40.0 °C-40.0 °F
Pour Point -40.0 °C-40.0 °FASTM D97

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WDUPJ803 / 253991

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.