MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

LATI Latilub 66-01M PA66, Molybdenum disulphide Filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, MoS2 Filled

Material Notes: Self-lubricating product based on Polyamide 66 (PA66). Molybdenum disulphide.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Information provided by Lati Industria Termoplastici S.p.A.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.14 g/cc0.0412 lb/in³
Linear Mold Shrinkage, Flow 0.012 - 0.015 cm/cm0.012 - 0.015 in/in
Linear Mold Shrinkage, Transverse 0.0125 - 0.0155 cm/cm0.0125 - 0.0155 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 85.0 MPa12300 psi
Elongation at Break 11 %11 %
Elongation at Yield 9.0 %9.0 %
Tensile Modulus 3.70 GPa537 ksi
Charpy Impact Unnotched NBNB
Charpy Impact, Notched 0.400 J/cm²1.90 ft-lb/in²
Coefficient of Friction, Dynamic 0.270.27
Coefficient of Friction, Static 0.290.29
K (wear) Factor 70.0 x 10-8 mm³/N-M34.7 x 10-10 in³-min/ft-lb-hr
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 235 °C455 °F
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C194 °F
Vicat Softening Point 240 °C
@Load 5.00 kg
464 °F
@Load 11.0 lb
Flammability, UL94 HB
@Thickness 0.750 mm
HB
@Thickness 0.0295 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 260 - 290 °C500 - 554 °F
Mold Temperature 70.0 - 90.0 °C158 - 194 °F
Drying Temperature 90.0 - 100 °C
@Time 10800 sec
194 - 212 °F
@Time 3.00 hour
 
Descriptive Properties
ISO Shrinkage - Pressure60 MPa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LATI Latilub 66-01M G/15 PA66, 15% Glass Fiber Reinforced, Molybdenum disulphide Filled
LG Chemical AF312A ABS, Flame Retardant
Mitsubishi Chemical Advanced Materials Nylatron® GS Nylon, Extruded MoS2 Filled Type 66 (ASTM Product Data Sheet)
A. Schulman ComAlloy Lubrilon® 602 Nylon 6/6, Molybdenum Disulfide Filled, Flow Enhanced
Overview of materials for Nylon 66, Glass Fiber/PTFE Filled

PLATH9863 / 177559

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.