MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Evonik VESTORAN® 1900 S27024 Polyphenylene Ether, Impact Grade
Categories: Polymer; Thermoplastic; Polyphenylene Ether/PPO; Polyphenylene Ether, Impact Grade

Material Notes: Unfilled, amorphous PPE resin. As a material of amorphous structure VESTORAN® 1900 S27024 shows very small mold shrinkage. Therefore molded parts have a very low tendency to warp. The impact modified compound is of low density and easy to process. Further properties are excellent impact strength, heat deflection under load and suitability for being coated with lacquers. Moldings of VESTORAN® 1900 S27024 are dimensionally stable and hydrolysis resistant even in hot water, but are more sensitive to organic solvents than semi-crystalline plastics. VESTORAN® 1900 S27024 is resistant to aqueous alkalines and acids, certain alcohols, and glycol solutions and particularly suitable for the adhesion promoter-free manufacturing of plastic/ rubber composites by the Evonik Industries AG -patented K&K process. VESTORAN® 1900 S27024 is supplied as cylindrical granules in PE-bags. Pigmentation may affect values.

Property data for dry samples.

Information provided by Evonik.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.04 g/cc0.0376 lb/in³ISO 1183
Linear Mold Shrinkage 0.0080 cm/cm0.0080 in/inNominal; ISO 294-4, 2577
Linear Mold Shrinkage, Flow 0.0090 cm/cm0.0090 in/inISO 294-4, 2577
Melt Flow 40 g/10 min
@Load 21.6 kg,
Temperature 300 °C
40 g/10 min
@Load 47.6 lb,
Temperature 572 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 53.0 MPa7690 psiISO 527
Tensile Strength 60.0 MPa8700 psiISO 527
Tensile Strength, Yield 60.0 MPa8700 psiISO 527
Elongation at Break >= 50 %>= 50 %Nominal; ISO 527
Elongation at Yield 5.0 %5.0 %ISO 527
Tensile Modulus 2.00 GPa290 ksiISO 527
Flexural Modulus 2.40 GPa348 ksiISO 178
Charpy Impact Unnotched 25.0 J/cm²
@Temperature 23.0 °C
119 ft-lb/in²
@Temperature 73.4 °F
Partial Break; ISO 179/1eU
Charpy Impact, Notched 2.50 J/cm²
@Temperature 23.0 °C
11.9 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+13 ohm-cm1.00e+13 ohm-cmIEC 62631-3-1
Dielectric Constant  2.6
@Frequency 100 Hz
2.6
@Frequency 100 Hz
IEC 62631-2-1
 2.9
@Frequency 1e+6 Hz
2.9
@Frequency 1e+6 Hz
IEC 62631-2-1
Dielectric Strength 40.0 kV/mm1020 kV/inAC, S20/P50; Sim. to IEC 60243-1
Dissipation Factor  0.0080
@Frequency 100 Hz
0.0080
@Frequency 100 Hz
IEC 62631-2-1
 0.016
@Frequency 1e+6 Hz
0.016
@Frequency 1e+6 Hz
IEC 62631-2-1
Comparative Tracking Index 200 V200 Vtest solution A, 100 drops value; IEC 60112
 225 V225 Vtest solution A, 50 drops value; IEC 60112
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 190 °C374 °FISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 170 °C338 °FISO 75-1/-2
Vicat Softening Point 185 °C365 °FMethod B: 10 N, 50 K/h; ISO 306
 190 °C374 °FMethod A: 10 N, 50 K/h; ISO 306
Flammability Test  1.0
@Thickness 0.800 mm
1.0
@Thickness 0.0315 in
IEC 60695-11-10
 5.0
@Thickness 1.60 mm
5.0
@Thickness 0.0630 in
IEC 60695-11-10
 
Processing PropertiesMetricEnglishComments
Mold Temperature 80.0 °C176 °FTest condition for mold shrinkage

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEVONIK889 / 243096

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.