MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Polyram Polytron P50B07 Polypropylene, 50% Long Glass Fiber, UV Stabilized
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 50% Glass Fiber Filler

Material Notes: A chemically coupled 50% long glass fiber reinforced black polypropylene, heat stabilized, UV stabilized for injection molding applications.

Information provided by Polyram.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.31 g/cc0.0473 lb/in³ISO 1183
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 135 MPa19600 psiISO 527
Elongation at Break 1.7 %1.7 %ISO 527
Tensile Modulus 12.9 GPa1870 ksiISO 527
Flexural Strength 210 MPa30500 psiISO 178
Flexural Modulus 11.0 GPa1600 ksiISO 178
Izod Impact, Notched (ISO) 25.0 kJ/m²11.9 ft-lb/in²ISO 180
Charpy Impact Unnotched 7.00 J/cm²33.3 ft-lb/in²ISO 179
Charpy Impact, Notched 2.20 J/cm²10.5 ft-lb/in²ISO 179
 
Thermal PropertiesMetricEnglishComments
Melting Point 167 °C333 °FISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 159 °C318 °FISO 75
Flammability, UL94 HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in
Flame Spread 20 mm/min0.79 in/minFMVSS302

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Techmer ES HiFill® PP LGF50 CC NAT 12mm 50% Glass Filled
Polyram RamOfin PPH308G50 Polypropylene, 50% Glass Fiber, Impact Modified
Polyram RamOfin PPC371B50 Polypropylene, 50% Mineral Filled
PlastiComp Complet® LGF50 - PP Homopolymer Polypropylene, 50% Long Glass Fiber Reinforced
Overview of materials for Polypropylene with 50% Glass Fiber Filler

PPOLYR946 / 126743

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.