MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ascend Performance Materials Vydyne® B 60 GF BK EST KW2 PA6-GF60
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 60% Glass Fiber Filled

Material Notes: Vydyne B 60 GF BK EST KW2 is standard flow, organic heat stabilized, 60% glass-fiber reinforced PA6 resin. Available in black, this product is also lubricated for improved machine feed and flow.

Information provided by Ascend Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.69 g/cc0.0611 lb/in³DAM; ISO 1183
Water Absorption 1.0 %
@Time 86400 sec
1.0 %
@Time 24.0 hour
DAM; ISO 62
Moisture Absorption at Equilibrium 1.1 %1.1 %DAM to 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0040 cm/cm
@Thickness 2.00 mm
0.0040 in/in
@Thickness 0.0787 in
DAM; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0050 cm/cm
@Thickness 2.00 mm
0.0050 in/in
@Thickness 0.0787 in
DAM; ISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 159 MPa23100 psi50% RH; ISO 527-2
 226 MPa32800 psiDAM; ISO 527-2
Elongation at Break 2.0 %2.0 %DAM; ISO 527-2
 3.7 %3.7 %50% RH; ISO 527-2
Tensile Modulus 14.8 GPa2150 ksi50% RH; ISO 527-2
 21.2 GPa3070 ksiDAM; ISO 527-2
Flexural Strength 245 MPa35500 psi50% RH; ISO 178
 371 MPa53800 psiDAM; ISO 178
Flexural Modulus 14.8 GPa2150 ksi50% RH; ISO 178
 21.5 GPa3120 ksiDAM; ISO 178
Poissons Ratio 0.320.32ISO 527-2
Izod Impact, Notched (ISO)  17.0 kJ/m²
@Temperature -40.0 °C
8.09 ft-lb/in²
@Temperature -40.0 °F
50% RH; ISO 180/1A
 17.0 kJ/m²
@Temperature -40.0 °C
8.09 ft-lb/in²
@Temperature -40.0 °F
DAM; ISO 180/1A
 17.0 kJ/m²
@Temperature -30.0 °C
8.09 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 180/1A
 17.0 kJ/m²
@Temperature 23.0 °C
8.09 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 180/1A
 18.0 kJ/m²
@Temperature -30.0 °C
8.57 ft-lb/in²
@Temperature -22.0 °F
50% RH; ISO 180/1A
 21.0 kJ/m²
@Temperature 23.0 °C
9.99 ft-lb/in²
@Temperature 73.4 °F
50% RH; ISO 180/1A
Charpy Impact Unnotched  8.70 J/cm²
@Temperature -40.0 °C
41.4 ft-lb/in²
@Temperature -40.0 °F
50% RH; ISO 179/1eU
 8.70 J/cm²
@Temperature -30.0 °C
41.4 ft-lb/in²
@Temperature -22.0 °F
50% RH; ISO 179/1eU
 8.80 J/cm²
@Temperature -40.0 °C
41.9 ft-lb/in²
@Temperature -40.0 °F
DAM; ISO 179/1eU
 8.80 J/cm²
@Temperature -30.0 °C
41.9 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 179/1eU
 8.80 J/cm²
@Temperature 23.0 °C
41.9 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 179/1eU
 9.00 J/cm²
@Temperature 23.0 °C
42.8 ft-lb/in²
@Temperature 73.4 °F
50% RH; ISO 179/1eU
Charpy Impact, Notched  1.70 J/cm²
@Temperature -40.0 °C
8.09 ft-lb/in²
@Temperature -40.0 °F
50% RH; ISO 179/1eA
 1.70 J/cm²
@Temperature -40.0 °C
8.09 ft-lb/in²
@Temperature -40.0 °F
DAM; ISO 179/1eA
 1.70 J/cm²
@Temperature -30.0 °C
8.09 ft-lb/in²
@Temperature -22.0 °F
50% RH; ISO 179/1eA
 1.70 J/cm²
@Temperature -30.0 °C
8.09 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 179/1eA
 1.70 J/cm²
@Temperature 23.0 °C
8.09 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 179/1eA
 2.10 J/cm²
@Temperature 23.0 °C
9.99 ft-lb/in²
@Temperature 73.4 °F
50% RH; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength  25.0 kV/mm
@Thickness 1.00 mm
635 kV/in
@Thickness 0.0394 in
50% RH; IEC 60243
 26.0 kV/mm
@Thickness 1.00 mm
660 kV/in
@Thickness 0.0394 in
DAM; IEC 60243
Comparative Tracking Index 575 V
@Thickness 3.00 mm
575 V
@Thickness 0.118 in
IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 13.0 µm/m-°C
@Thickness 2.00 mm,
Temperature 35.0 - 55.0 °C
7.22 µin/in-°F
@Thickness 0.0787 in,
Temperature 95.0 - 131 °F
DAM; ISO 11359-2
CTE, linear, Transverse to Flow 69.0 µm/m-°C
@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
38.3 µin/in-°F
@Thickness 0.0787 in,
Temperature 73.4 - 131 °F
DAM; ISO 11359-2
Melting Point 220 °C428 °FDAM; ISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 217 °C423 °FUnannealed; 50% RH; ISO 75-2/B
 220 °C428 °FUnannealed; DAM; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 208 °C406 °FUnannealed; 50% RH; ISO 75-2/A
 214 °C417 °FUnannealed; DAM; ISO 75-2/A
Flammability, UL94  HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
 HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 230 - 280 °C446 - 536 °FInjection
Middle Barrel Temperature 230 - 280 °C446 - 536 °FInjection
Front Barrel Temperature 230 - 280 °C446 - 536 °FInjection
Nozzle Temperature 230 - 280 °C446 - 536 °FInjection
Melt Temperature 230 - 280 °C446 - 536 °FInjection
Mold Temperature 80.0 - 90.0 °C176 - 194 °FInjection
Drying Temperature 80.0 - 90.0 °C176 - 194 °FInjection
Dry Time >= 3.00 hour>= 3.00 hourInjection
 
Descriptive Properties
AdditiveHeat Stabilizer
 Lubricant
AppearanceBlack
FeaturesChemical Resistant
 Gasoline Resistant
 General Purpose
 Good Flow
 Good Heat Resistance
 Lubricated
 Organic Heat Stabilized
FormsPellets
Processing MethodInjection Molding
RegionNorth America, Europe, Asia Pacific

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PASCE9284 / 287637

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.