MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Nylon

Nylacast Moly Cast Nylon 6, MoS2 Filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, MoS2 Filled

Material Notes: Nylacast Moly is a cast nylon material in which improved crystallisation occurs by the addition of Molybdenum Disulphide. On account of this the superficial hardness increases (providing excellent machine ability) and simultaneously the general mechanical and anti-friction properties are improved. Due to the fact that the crystal structure breaks down immediately before the melting temperature is reached, the thermal properties of the material are improved over the basic grade. MoS2 provides a degree of self lubrication leading to an improvement in the wear properties of the material. These improved properties, combined with lower water absorption, extend the range of applications that Moly has over Natural cast nylon. Dynamic bearing applications at elevated operating temperatures of up to 105ºC are particularly suited to this material.

Benefits:

  • Increased superficial hardness provides excellent machine ability
  • Improvement in wear properties as a result of dry lubricant
  • Improved anti-friction properties
  • Improved mechanical properties
  • Elevated operating temperatures
  • Lower water absorption
  • Improved dimensional stability
  • Excellent chemical resistance properties
  • Good PV and load bearing capabilities
  • Extended range of applications
Typical Application:
  • Sheaves
  • Wear pads
  • Rollers
  • Bearings
  • Spacers
  • Bush
  • Slide pads
  • Chain Wheel
  • Chain sheaves
  • Hose Clamp
  • Wear strips
  • Wear plates
  • Spacer
  • Bespoke Components

Information provided by Nylacast Ltd.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.15 g/cc0.0415 lb/in³method A; ISO 1183:1987
Water Absorption 0.20 %
@Time 86400 sec
0.20 %
@Time 24.0 hour
Immersion; ISO 62:1999
Moisture Absorption at Equilibrium 2.1 %2.1 %50% RH, 23°C; ISO 62:1999
Water Absorption at Saturation 6.3 %
@Time 86400 sec
6.3 %
@Time 24.0 hour
Immersion @ 23°C; ISO 62:1999
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8080ISO 868:2003
Tensile Strength, Yield 75.0 - 80.0 MPa10900 - 11600 psiSample Type 1B, 50mm/min; ISO 527-1/2:1993
Elongation at Break >= 20 %>= 20 %Type 1B, 50mm/min; ISO 527-1/2:1993
Tensile Modulus 3.80 - 4.00 GPa551 - 580 ksiE-modulus; Type 1B, 50mm/min; ISO 527-1/2:1993
Flexural Strength 100 - 110 MPa14500 - 16000 psi1.5mm/min; ISO 178:2001
Flexural Modulus 3.00 - 3.20 GPa435 - 464 ksi1.5mm/min; ISO 178:2001
Compressive Strength 105 MPa15200 psiType B, 5mm/min; ISO 604:2002
Compressive Modulus 2.50 - 2.70 GPa363 - 392 ksiType B, 5mm/min; ISO 604:2002
Izod Impact, Notched (ISO) 5.50 - 7.00 kJ/m²2.62 - 3.33 ft-lb/in²Type A; ISO 180:2000
Coefficient of Friction, Dynamic 0.10
@Pressure 1.75 MPa
0.10
@Pressure 254 psi
31.4m/min
K Factor (Wear Factor) 220000
@Pressure 1.75 MPa
220000
@Pressure 254 psi
[m3/Nm], 31.4m/min
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cmIEC 60093:1980-01
Surface Resistance >= 1.00e+14 ohm>= 1.00e+14 ohmIEC 60093:1980-01
Dielectric Constant  3.7
@Frequency 1e+6 Hz
3.7
@Frequency 1e+6 Hz
IEC 60250:1969-01
 4.0
@Frequency 100 Hz
4.0
@Frequency 100 Hz
IEC 60250:1969-01
Dielectric Strength 25.0 kV/mm635 kV/inIEC 60243-1:1998-01
Dissipation Factor 0.11
@Frequency 100 Hz
0.11
@Frequency 100 Hz
IEC 60250:1969-01
Comparative Tracking Index 600 V600 VIEC 60112:2003-01
 
Thermal PropertiesMetricEnglishComments
CTE, linear 85.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
47.2 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-2:1999
Thermal Conductivity 0.280 W/m-K1.94 BTU-in/hr-ft²-°FMean T = 20°C; ISO 8301:1991
Melting Point 221 °C430 °F
Maximum Service Temperature, Air 170 °C338 °FIntermittent
 105 °C
@Time 1.80e+7 sec
221 °F
@Time 5000 hour
Continuous
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C194 °FISO 75
Minimum Service Temperature, Air -100 °C-148 °FIntermittent
 -40.0 °C-40.0 °FContinuous
Glass Transition Temp, Tg 68.0 °C154 °FISO 11359:1999
Flammability, UL94 HBHBIEC 60695-11-10:2003-08
 
Descriptive Properties
ColorBlack
Limiting PV100 MPa/m

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultramid® B3EG6 30% Glass Filled PA6 (Dry)
Aluminum Bronze, UNS C95400, Copper Casting Alloy, TQ50 Temper
Delrin Delrin® 100 NC010 POM
Mitsubishi Chemical Advanced Materials Nylatron® MC 901 H. S. Type 6 (ASTM Product Data Sheet)
GEHR Plastics PA 6 Nylon 6, Dry

PNYLAC02 / 89260

Nylon

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.