MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Mocom (ALBIS) ALCOM® LD MABS 1000 15012 GN1023-15 MABS
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded

Material Notes: Base Polymer: Methylmethacrylate Acrylonitrile Butadiene Styrene

Filler/Additive System: 40% mineral

Special Features: Highly reflective, opaque, low emission

Market Segment: Automotive, Lighting

Application Area: Lighting, light blocking components

Typical Application: Light guides, reflectors

Information provided by Albis Plastics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.07 g/cc0.0387 lb/in³ISO 1183
Melt Flow 8.0 g/10 min
@Load 10.0 kg,
Temperature 220 °C
8.0 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 74.0 MPa10700 psiH358/30; ISO 2039-1
Tensile Strength 40.0 MPa5800 psiISO 527
Tensile Strength, Yield 41.0 MPa5950 psiISO 527
Elongation at Break 20 %20 %ISO 527
Elongation at Yield 4.0 %4.0 %ISO 527
Tensile Modulus 1.80 GPa261 ksiISO 527
Flexural Strength 57.0 MPa8270 psiISO 178
 53.0 MPa
@Strain 3.5 %
7690 psi
@Strain 3.5 %
ISO 178
Flexural Modulus 1.90 GPa276 ksiISO 178
Charpy Impact Unnotched  6.00 J/cm²
@Temperature -40.0 °C
28.6 ft-lb/in²
@Temperature -40.0 °F
ISO 179/1eU
 14.0 J/cm²
@Temperature 23.0 °C
66.6 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched  0.200 J/cm²
@Temperature -40.0 °C
0.952 ft-lb/in²
@Temperature -40.0 °F
ISO 179/1eA
 0.500 J/cm²
@Temperature 23.0 °C
2.38 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 76.0 °C169 °FISO 75-1/-2
Vicat Softening Point 87.0 °C189 °FB50; ISO 306
Flammability, UL94  HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
 HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in
 
Optical PropertiesMetricEnglishComments
Haze  95.5 %
@Thickness 1.00 mm
95.5 %
@Thickness 0.0394 in
A,2°; ISO 13468
 95.5 %
@Thickness 2.00 mm
95.5 %
@Thickness 0.0787 in
A,2°; ISO 13468
 95.5 %
@Thickness 3.00 mm
95.5 %
@Thickness 0.118 in
A,2°; ISO 13468
 95.5 %
@Thickness 4.00 mm
95.5 %
@Thickness 0.157 in
A,2°; ISO 13468
Transmission, Visible  6.5 %
@Thickness 4.00 mm
6.5 %
@Thickness 0.157 in
A,2°; ISO 13468
 11 %
@Thickness 3.00 mm
11 %
@Thickness 0.118 in
A,2°; ISO 13468
 20.5 %
@Thickness 2.00 mm
20.5 %
@Thickness 0.0787 in
A,2°; ISO 13468
 43 %
@Thickness 1.00 mm
43 %
@Thickness 0.0394 in
A,2°; ISO 13468
 
Processing PropertiesMetricEnglishComments
Melt Temperature 230 - 260 °C446 - 500 °FInjection molding
Mold Temperature 50.0 - 80.0 °C122 - 176 °FInjection molding
Drying Temperature  70.0 °C
@Time 3600 - 10800 sec
158 °F
@Time 1.00 - 3.00 hour
in a dry air (desiccant) dryer
 70.0 °C
@Time 7200 - 14400 sec
158 °F
@Time 2.00 - 4.00 hour
in an circulating dryer
 
Descriptive Properties
Base PolymerMethylmethacrylate Acrylonitrile Butadiene Styrene
Half Power Angle31°d=1mm, A,2°
 49°d=2mm, A,2°
 53°d=3mm, A,2°
 55°d=4mm, A,2°

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Trinseo Plexiglas® MI7 Acrylic

PALBIS8463 / 242522

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.