MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

410 Cb Martensitic Stainless Steel (UNS S41040)
Categories: Metal; Ferrous Metal; Martensitic; Stainless Steel; T 400 Series Stainless Steel

Material Notes: Fe-11.9Cr-0.24Si-0.19Mn-0.15Nb-0.12C-0.027Mo-0.021P-0.04S

Typically used for molds, bearings, turbine components, aircraft structural parts, medical instruments, and cutlery

Key Words: UNS S41040
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.73 g/cc0.279 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B >= 89>= 89
Hardness, Rockwell C <= 32<= 32
Tensile Strength, Ultimate 655 - 1248 MPa95000 - 181000 psi
Tensile Strength, Yield 503 - 1034 MPa
@Strain 0.2 %
73000 - 150000 psi
@Strain 0.2 %
Elongation at Break 15 - 26 %15 - 26 %
Modulus of Elasticity 204 - 215 GPa29600 - 31200 ksi
Bulk Modulus 166 GPa24100 ksi
Poissons Ratio 0.2830.283
Shear Modulus 83.9 GPa12200 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000570 ohm-cm0.0000570 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear >= 9.90 µm/m-°C>= 5.50 µin/in-°F
Specific Heat Capacity 0.460 J/g-°C0.110 BTU/lb-°F
Thermal Conductivity 24.8 W/m-K172 BTU-in/hr-ft²-°F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.12 %0.12 %
Chromium, Cr 11.9 %11.9 %
Iron, Fe 87.312 %87.312 %As Balance
Manganese, Mn 0.19 %0.19 %
Molybdenum, Mo 0.027 %0.027 %
Niobium, Nb (Columbium, Cb) 0.15 %0.15 %
Phosphorus, P 0.021 %0.021 %
Silicon, Si 0.24 %0.24 %
Sulfur, S 0.040 %0.040 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
410 Stainless Steel
AISI Type 410S Stainless Steel
410 Stainless Steel, tempered at 233°C
405 Stainless Steel, annealed, bar
420 Stainless Steel

MQ410E / 100240

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.