MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Dow Appeel® 20D828 Ethylene Acrylate
Categories: Polymer; Thermoplastic; Ethylene Acrylic Acid

Material Notes: Appeel® 20D828 is an modified ethylene acrylate resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide strong peelable seals over a broad temperature range to a number of container materials including PP, PS, PP, PVC, Aclar®, Barex®, and certain epoxy coatings. Appeel® 20D828 is available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylene resins.

Appeel® 20D828 Lidding Sealant Resin complies with Food and Drug Administration Regulation 21 CFR 175.320 – Resinous and polymeric coatings for polyolefin films, subject to the limitations and requirements therein. This regulation describes resinous and polymeric coatings for polyolefin films that may be used in contact with food under Conditions of Use C through H (as described in Table 2 of 21 CFR 176.170(c), subject to the finished food-contact article meeting the extractive limitations under the intended conditions of use, as shown in paragraph (c ) of the Regulation.

This former DuPont product line is now a Dow product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.02 g/cc0.0368 lb/in³ASTM D792, ISO 1183
Melt Flow 13 g/10 min
@Load 2.16 kg,
Temperature 190 °C
13 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238, ISO 1133
 
Thermal PropertiesMetricEnglishComments
Melting Point 97.0 °C207 °FASTM D3418, ISO 3146
Vicat Softening Point 58.0 °C136 °FASTM D1525, ISO 306
 
Processing PropertiesMetricEnglishComments
Processing Temperature <= 240 °C<= 464 °F
Feed Temperature 140 °C284 °FBlown Film Coextrusion
 160 °C320 °FExtrusion Coating
Zone 2 150 °C302 °FBlown Film Coextrusion
 185 °C365 °FExtrusion Coating
Zone 3 160 °C320 °FBlown Film Coextrusion
 210 °C410 °FExtrusion Coating
Zone 4 180 °C356 °FBlown Film Coextrusion
 235 °C455 °FExtrusion Coating
Zone 5 180 °C356 °FBlown Film Coextrusion
 235 °C455 °FExtrusion Coating
Adapter Temperature 180 °C356 °FBlown Film Coextrusion
 235 °C455 °FExtrusion Coating
Die Temperature 170 °C338 °FBlown Film Coextrusion
 235 °C455 °FExtrusion Coating
Melt Temperature 150 - 190 °C302 - 374 °FBlown Film Coextrusion
 180 - 240 °C356 - 464 °FExtrusion Coating
Dry Time 5.00 hour
@Temperature 55.0 °C
5.00 hour
@Temperature 131 °F
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow Appeel® 20D784 Ethylene Acrylate
Dow Appeel® 20D855 Ethylene Acrylate
Dow Appeel® 22D843 Ethylene Acrylate
BASF Paliotol™ Yellow K 1700 Color Additive
Dow Appeel® 20D875 Ethylene Acrylate

PDTA4903 / 170343

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.