MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Murtfeldt Murflor® + Bronze Polytetrafluoroethylene, 60% Bronze
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE); Polytetrafluoroethylene (PTFE), Bronze Filled

Material Notes: The addition of 60% bronze to the base material reduces the expansion coefficient and gives lower sliding wear.

Special Properties:
• Lower sliding wear than Murflor®
• Good slide properties
• Low stick/slip effect
• Higher compressive strength than Murflor®

Information provided by Murtfeldt Kunststoffe GmbH & Co. KG.

Key Words: PTFE CuSn
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 3.88 g/cc0.140 lb/in³ISO 1183-1
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6868DIN 53505
Tensile Strength, Yield 14.0 MPa2030 psiISO 527-1/-2
Elongation at Break 140 %140 %ISO 527-1/-2
Modulus of Elasticity 1.38 GPa200 ksi
Compressive Yield Strength 10.5 MPa
@Strain 1 %
1520 psi
@Strain 1 %
dry; ISO 604
Charpy Impact, Notched 1.10 J/cm²5.23 ft-lb/in²ISO 179-1/1eA
Coefficient of Friction, Dynamic 0.140.14
Sand Slurry 0.500.50µm/km
 
Electrical PropertiesMetricEnglishComments
Surface Resistance >= 1.00e+13 ohm>= 1.00e+13 ohm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 95.0 µm/m-°C
@Temperature 23.0 - 100 °C
52.8 µin/in-°F
@Temperature 73.4 - 212 °F
Melting Point 330 °C626 °FISO 11357-1
Maximum Service Temperature, Air  260 °C
@Time 7.20e+7 sec
500 °F
@Time 20000 hour
 300 °C
@Time <=86400 sec
572 °F
@Time <=24.0 hour
Minimum Service Temperature, Air -200 °C-328 °F
Glass Transition Temp, Tg 127 °C261 °FISO 11357-1
Flammability, UL94 V-0V-0
 
Compliance PropertiesMetricEnglishComments
FDA NoNo
 
Descriptive Properties
ColorBronze

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Sandvik Osprey 90/10 Cu Sn Powder (Grade 95% - 16)
Carlson 90 10 Cu Ni Copper-Nickel Alloy
Sandvik Osprey 90/10 Cu Sn Powder (Grade 90% - 22)
Sandvik Osprey 85/15 Cu Sn Powder (Grade 80% - 22)
302 Stainless Steel, annealed bar

PMURT936 / 156583

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.