MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Borealis FR4850 Polypropylene, Flame Retardant
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Flame Retardant

Material Notes: FR4850 is a halogen free flame retardant polypropylene compound for Primary Automotive Wire.

Applications: FR4850 is intended for use as a 125°C rated primary insulation for automotive wires from 0.35 mm² or 22 AWG up to 1.5 mm² or 16 AWG Specifications: FR4850 meets the applicable requirements as below when processed using sound extrusion practice and testing procedure

  • SAE J1128/J1127
  • GMW15626
  • Chrysler MS-12441
  • Ford ES-AU5T-1A348-AA
  • ISO 6722

Information provided by Borealis AG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.38 g/cc0.0499 lb/in³Compound; ISO 1872-2/ISO 1183
Melt Flow 1.00 g/10 min
@Load 2.16 kg,
Temperature 230 °C
1.00 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Storage Temperature 10.0 - 30.0 °C50.0 - 86.0 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 70.070.0ISO 868
Tensile Strength >= 15.0 MPa>= 2180 psiIEC 60811-501
 >= 7.50 MPa
@Treatment Temp. 165 °C,
Time 605000 sec
>= 1090 psi
@Treatment Temp. 329 °F,
Time 168 hour
after aging; SAE J1128
Elongation at Break >= 300 %>= 300 %IEC 60811-501
 >= 150 %
@Treatment Temp. 165 °C,
Time 605000 sec
>= 150 %
@Treatment Temp. 329 °F,
Time 168 hour
SAE J1128
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 3.00
@Frequency 50 Hz
3.00
@Frequency 50 Hz
IEC 250
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature <= -40.0 °C<= -40.0 °FISO 6722
Oxygen Index 27.0 %27.0 %Limiting; ISO 4589-2
 
Processing PropertiesMetricEnglishComments
Drying Temperature 50.0 - 80.0 °C122 - 176 °F
Dry Time 4.00 - 12.0 hour4.00 - 12.0 hour
Shelf Life 24.0 Month24.0 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBORE9777 / 323134

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.