System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Borealis CG9620 High Density Polyethylene
Categories:
Polymer
;
Film
;
Thermoplastic
;
Polyethylene (PE)
;
High Density (HDPE)
;
High Density Polyethylene (HDPE), Film Grade
Material Notes:
CG9620 is a high density polyethylene film grade which combine excellent extrusion behavior with superior mechanical properties. Applications: CG9620 is recommended for coated film and co-extrusion applications.
Information provided by Borealis AG
Key Words:
PE
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
0.962
g/cc
0.0348
lb/in³
ISO 1183
Melt Flow
12
g/10 min
@Load 2.16 kg,
Temperature 190 °C
12
g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Coating Weight
9.00
g/m²
5.63
lb/ream
BTM 14922
Thermal Properties
Metric
English
Comments
Melting Point
131
°C
268
°F
DSC; ISO 3146
Descriptive Properties
Coating Speed (m/min)
> 400 m/min
BTM 14921
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Borealis Borstar® FB1460 HDPE for Film
Overview of materials for High Density Polyethylene (HDPE), Film Grade
Borealis CA7230 Low Density Polyethylene
Chevron Phillips HiD® 9605D HDPE Cast Film Resin
Chevron Phillips Marlex® 9608XD HDPE Film Grade
PBOREA399 / 108658
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.