MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

Ensinger Tecapeek® black Polyetheretherketone
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Unreinforced

Material Notes:
  • made exclusively from Victrex® resin
  • excellent chemical resistance
  • high thermal resistance
  • good heat deflection temperature
  • good machinability
  • very good slide and wear properties
  • hydrolysis and superheated steam
  • resistant
Target Industries:
  • aircraft and aerospace technology
  • oil and gas industry
  • chemical plant engineering
  • semiconductor technology
  • food engineering
  • medical technology
  • automotive industry
  • process engineering
  • mechanical engineering

Information provided by Ensinger Inc.

Vendors: Ensinger TECAPEEK™ shapes are manufactured exclusively with Victrex™ PEEK polymer. The Ensinger process and Victrex resins ensure reliability, consistency, dimensional stability, and high temperature mechanical performance.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.31 g/cc0.0473 lb/in³
Moisture Absorption 0.450 %0.450 %saturation; DIN EN ISO 62
 0.0200 %
@Time 86400 sec
0.0200 %
@Time 24.0 hour
ASTM D 570
Storage Temperature 10.0 - 37.8 °C50.0 - 100 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 9999ASTM D 785
Tensile Strength at Break 53.8 MPa7800 psiASTM D 638
Tensile Strength, Yield 110 MPa16000 psiASTM D 638
Elongation at Break 40 %40 %ASTM D 638
Elongation at Yield 4.9 %4.9 %ASTM D 638
Modulus of Elasticity 4.48 GPa650 ksiASTM D 638
Flexural Strength 179 MPa26000 psiASTM D 790
Flexural Modulus 4.14 GPa600 ksiASTM D 790
Compressive Yield Strength 121 MPa
@Strain 10 %
17500 psi
@Strain 10 %
ASTM D 695
Compressive Modulus 3.40 GPa493 ksiASTM D 695
Izod Impact, Notched 0.507 J/cm0.950 ft-lb/inASTM D 256
Coefficient of Friction, Dynamic 0.25
@Pressure 0.276 MPa
0.25
@Pressure 40.0 psi
50 fpm; ASTM D 3702
Coefficient of Friction, Static 0.20
@Pressure 0.276 MPa
0.20
@Pressure 40.0 psi
ASTM D 3702
K (wear) Factor 403 x 10-8 mm³/N-M200 x 10-10 in³-min/ft-lb-hr40 psi, 50 fpm; ASTM D 3702
Limiting Pressure Velocity 2.42 MPa-m/sec69000 psi-ft/minASTM D 3702
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 4.90e+16 ohm-cm4.90e+16 ohm-cmASTM D 149
Surface Resistivity per Square 1.00e+16 ohm1.00e+16 ohmASTM D 257
Dielectric Constant 2.8
@Frequency 1000 Hz
2.8
@Frequency 1000 Hz
DIN IEC 60250
Dielectric Strength 24.8 kV/mm
@Thickness 2.54 mm
630 kV/in
@Thickness 0.100 in
IEC 60243-1
Dissipation Factor 0.0030
@Frequency 1e+6 Hz
0.0030
@Frequency 1e+6 Hz
DIN IEC 60250
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 45.0 µm/m-°C25.0 µin/in-°F< Tg; DIN EN ISO 11359-1;2
Thermal Conductivity 0.290 W/m-K2.01 BTU-in/hr-ft²-°FISO 22007-4:2008
Melting Point 334 °C633 °F
Maximum Service Temperature, Air 249 °C480 °FLong Term
 300 °C572 °FShort Term
Deflection Temperature at 1.8 MPa (264 psi) 160 °C320 °FASTM D 648
Glass Transition Temp, Tg 150 °C302 °FDIN EN ISO 11357
Flammability, UL94 V-0V-0
 
Descriptive Properties
Colorblack opaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PENSIN8187 / 319115

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.