This premium H13 grade steel, produced via special melting and refining techniques possesses excellent toughness making it suitable for demanding hot work applications. W302 Superior meets or exceeds NADCA 207-97 and 207-2003 Superior Specification in dimensions 18" and greater in thickness. A premium grade H13 hot work tool steel featuring: - Very good toughness properties
- Very good heat checking resistance
- Good temper resistance and high temperature strength
- Excellent polishability and texturability
- Manufactured for flats greater than 18 inches in thickness
|
DIN 1.2344; JIS SKD61; 40CrMoV5 |