MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Mitsubishi Chemical Advanced Materials Extrulen® 1050 MediTECH Extruded UHMWPE Form
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); UHMW PE (Ultra High Molecular Weight PE)

Material Notes: MediTECH Extruded UHMWPE Form, produced from Celanese GUR 1050 resin. ISO Cell Designation: Thermoplastic ISO 11542-PE-UHMW QD, 2-2-2, ASTM Cell Designation: S-UHMW-PE0111A111 Material evaluated based on ISO 5834-1 Type 1, ISO 5834-2 Type 1, and ASTM F648 Type 1.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.931 g/cc0.931 g/ccASTM D792
Water Absorption <= 0.050 %<= 0.050 %ASTM D570
Oxidative Induction Time (OIT) 10 min10 minASTM D3895
Crystallinity 58 %58 %1st heat, 20°C - 160°C; ASTM F2625
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 66
@Time 15.0 sec
66
@Time 0.00417 hour
ASTM D2240
Tensile Strength, Ultimate 54.7 MPa7930 psiASTM F648 /ASTM D638
Tensile Strength, Yield 21.6 MPa3130 psiASTM F648 /ASTM D638
Elongation at Break 401 %401 %ASTM F648 /ASTM D638
Charpy Impact Unnotched 10.1 J/cm²48.1 ft-lb/in²ISO 11542-2
 
Thermal PropertiesMetricEnglishComments
CTE, linear 180 µm/m-°C
@Temperature 23.0 - 80.0 °C
100 µin/in-°F
@Temperature 73.4 - 176 °F
ASTM D696
Thermal Conductivity 0.400 W/m-K2.78 BTU-in/hr-ft²-°FDIN 52612
Melting Point 138 °C280 °F10°C / min; ASTM DF2625
Crystallization Temperature 126 - 144 °C259 - 291 °FASTM F2625
Deflection Temperature at 1.8 MPa (264 psi) 45.0 °C113 °FASTM D648
Vicat Softening Point 134 °C
@Load 1.02 kg
273 °F
@Load 2.25 lb
50 °C/Hr.; ASTM D1525 B
 
Descriptive Properties
Oxidation Resistance<0.1ASTM F2102, Surface Oxidation Index
 <0.1ASTM F2102, Bulk Oxidation Index

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

P1SM934 / 291091

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.