MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CENTROPLAST CENTROMID 12 GF 30 Polyamide 12 30% glass fiber
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12); Nylon 12, 30% Glass Fiber Filled

Material Notes: CENTROMID 12 GF 30 is a dimensionally stable and high strength material with good electrical insulating properties. Its applications include levers and valve parts.

Information provided by CENTROPLAST Engineering Plastics GMBH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.23 g/cc0.0444 lb/in³ISO 1183
Moisture Absorption at Equilibrium 0.60 %0.60 %in normal climate 23°C/50%RH; ISO 62
Water Absorption at Saturation 1.1 %1.1 %in water at 23°C; ISO 62
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 120 MPa17400 psivalue at 30 sec.; ISO 2039-1
Tensile Strength at Break 105 MPa15200 psiv = 5 mm/min; ISO 527-2
Elongation at Break 8.0 %8.0 %ISO 527-2
Tensile Modulus 6.00 GPa870 ksiISO 527-2
Charpy Impact Unnotched 8.00 J/cm²38.1 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 2.00 J/cm²9.52 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+13 ohm-cm1.00e+13 ohm-cmIEC 60093
Surface Resistance 1.00e+12 ohm1.00e+12 ohmIEC 60093
Dielectric Constant 4.0
@Frequency 1e+6 Hz
4.0
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 35.0 kV/mm889 kV/inin transformer oil; IEC 60243-1
Dissipation Factor 0.040
@Frequency 1e+6 Hz
0.040
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 V600 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear 20.0 µm/m-°C
@Temperature 20.0 °C
11.1 µin/in-°F
@Temperature 68.0 °F
ISO 11359
Thermal Conductivity 0.160 W/m-K1.11 BTU-in/hr-ft²-°F
Melting Point 178 °C352 °F10K/min; ISO 3146
Maximum Service Temperature, Air 150 °C302 °FShort term
 160 °C320 °FLong Term
Deflection Temperature at 1.8 MPa (264 psi) 160 °C320 °FISO 75-2
Flammability, UL94  HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in
 HB
@Thickness 6.00 mm
HB
@Thickness 0.236 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum 6061-T6; 6061-T651
Akro-Plastic Akrotek® PAEK CF 30 black (5216) PEKK, Dry, 30% Carbon Filled
Barlog Plastics KEBAFLEX P D35.1 Polyester-Elastomer, Shore D35
Barlog Plastics KEBAFLEX E 35.1 TPE-V, Shore A35
Barlog Plastics KEBAFLEX P D55.1 Polyester-Elastomer, Shore D55

PCENTR14 / 27965

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.