MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Bada BADAMID® PPA-HT CF15 TF20 H black PPA, 15% Carbon Fiber Reinforced, Dry
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA); Polyphthalamide (PPA), Carbon Fiber Filled

Material Notes: Heat stabilized injection molding grade based on PPA for tribological applications

Information provided by Bada

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.35 g/cc0.0488 lb/in³ISO 1183
Moisture Absorption 1.50 %1.50 %50% r.h.; ISO 62
Water Absorption at Saturation 5.0 %5.0 %ISO 62
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 180 MPa26100 psi5 mm/min; ISO 527-1/2
Elongation at Break 2.3 %2.3 %5 mm/min; ISO 527-1/2
Tensile Modulus 12.8 GPa1860 ksi1 mm/min; ISO 527-1/2
Charpy Impact Unnotched 5.00 J/cm²
@Temperature 23.0 °C
23.8 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 0.700 J/cm²
@Temperature 23.0 °C
3.33 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Surface Resistance <= 10000 ohm<= 10000 ohmIEC-62631-3-2
Comparative Tracking Index 100 V100 VIEC-60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 30.0 µm/m-°C16.7 µin/in-°FISO 11359-2
CTE, linear, Transverse to Flow 60.0 µm/m-°C33.3 µin/in-°FISO 11359-2
Maximum Service Temperature, Air 290 °C554 °Fsome hours; EC-60216
 150 °C
@Time 7.20e+7 sec
302 °F
@Time 20000 hour
EC-60216
Deflection Temperature at 0.46 MPa (66 psi) 290 °C554 °FISO 75-1/2
Deflection Temperature at 1.8 MPa (264 psi) 280 °C536 °FISO 75-1/2
Flammability, UL94  HB
@Thickness 0.750 mm
HB
@Thickness 0.0295 in
 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 330 - 350 °C626 - 662 °F
Mold Temperature >= 135 °C>= 275 °F
Drying Temperature 120 °C248 °F
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hour
Moisture Content <= 0.050 %<= 0.050 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBADA248 / 287081

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.