MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Envalior ForTii® T11 PPA-GF30 FR(40) PA4T High Temperature Polyamide
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA); Polyphthalamide (PPA), 30% Glass Fiber Reinforced

Material Notes: ForTii® is a high temperature polyamide for applications in the electronics, lighting, automotive, white goods, industrial and aerospace industries. ForTii® T11 has optimal toughness and is the best solution for (automotive) electrical components in harsh environments to minimize the risk of cracking and to provide design freedom and product reliability.

Features: Phosphorous free, VDE certified. 30% glass reinforced. Processing: Injection Molding.

Former DSM Engineering Plastics product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.46 g/cc0.0527 lb/in³Dry; ISO 1183
Moisture Absorption 1.60 %1.60 %Dry; Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0030 cm/cm0.0030 in/inDry; ISO 294-4
Linear Mold Shrinkage, Transverse 0.012 cm/cm0.012 in/inDry; ISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break  70.0 MPa
@Temperature 160 °C
10200 psi
@Temperature 320 °F
Dry; ISO 527-1/-2
 80.0 MPa
@Temperature 140 °C
11600 psi
@Temperature 284 °F
Dry; ISO 527-1/-2
 90.0 MPa
@Temperature 80.0 °C
13100 psi
@Temperature 176 °F
Cond; ISO 527-1/-2
 105 MPa
@Temperature 120 °C
15200 psi
@Temperature 248 °F
Dry; ISO 527-1/-2
 120 MPa
@Temperature 100 °C
17400 psi
@Temperature 212 °F
Dry; ISO 527-1/-2
 130 MPa
@Temperature 80.0 °C
18900 psi
@Temperature 176 °F
Dry; ISO 527-1/-2
 150 MPa
@Temperature 23.0 °C
21800 psi
@Temperature 73.4 °F
Cond; ISO 527-1/-2
 160 MPa
@Temperature 23.0 °C
23200 psi
@Temperature 73.4 °F
Dry; ISO 527-1/-2
 180 MPa
@Temperature -40.0 °C
26100 psi
@Temperature -40.0 °F
Dry; ISO 527-1/-2
Elongation at Break  2.1 %
@Temperature 23.0 °C
2.1 %
@Temperature 73.4 °F
Cond; ISO 527-1/-2
 2.1 %
@Temperature 80.0 °C
2.1 %
@Temperature 176 °F
Dry; ISO 527-1/-2
 2.1 %
@Temperature 100 °C
2.1 %
@Temperature 212 °F
Dry; ISO 527-1/-2
 2.2 %
@Temperature 23.0 °C
2.2 %
@Temperature 73.4 °F
Dry; ISO 527-1/-2
 2.3 %
@Temperature -40.0 °C
2.3 %
@Temperature -40.0 °F
Dry; ISO 527-1/-2
 2.9 %
@Temperature 120 °C
2.9 %
@Temperature 248 °F
Dry; ISO 527-1/-2
 3.2 %
@Temperature 80.0 °C
3.2 %
@Temperature 176 °F
Cond; ISO 527-1/-2
 3.6 %
@Temperature 140 °C
3.6 %
@Temperature 284 °F
Dry; ISO 527-1/-2
 4.5 %
@Temperature 160 °C
4.5 %
@Temperature 320 °F
Dry; ISO 527-1/-2
Tensile Modulus  5.00 GPa
@Temperature 160 °C
725 ksi
@Temperature 320 °F
Dry; ISO 527-1/-2
 5.70 GPa
@Temperature 140 °C
827 ksi
@Temperature 284 °F
Dry; ISO 527-1/-2
 7.60 GPa
@Temperature 80.0 °C
1100 ksi
@Temperature 176 °F
Cond; ISO 527-1/-2
 8.00 GPa
@Temperature 120 °C
1160 ksi
@Temperature 248 °F
Dry; ISO 527-1/-2
 10.0 GPa
@Temperature 100 °C
1450 ksi
@Temperature 212 °F
Dry; ISO 527-1/-2
 10.8 GPa
@Temperature 80.0 °C
1570 ksi
@Temperature 176 °F
Dry; ISO 527-1/-2
 11.5 GPa
@Temperature 23.0 °C
1670 ksi
@Temperature 73.4 °F
Dry; ISO 527-1/-2
 12.0 GPa
@Temperature 23.0 °C
1740 ksi
@Temperature 73.4 °F
Cond; ISO 527-1/-2
 12.0 GPa
@Temperature -40.0 °C
1740 ksi
@Temperature -40.0 °F
Dry; ISO 527-1/-2
Flexural Strength 230 MPa33400 psiCond; ISO 178
 255 MPa37000 psiDry; ISO 178
Flexural Modulus  5.00 GPa
@Temperature 160 °C
725 ksi
@Temperature 320 °F
Dry; ISO 178
 8.20 GPa
@Temperature 120 °C
1190 ksi
@Temperature 248 °F
Dry; ISO 178
 11.0 GPa
@Temperature 23.0 °C
1600 ksi
@Temperature 73.4 °F
Dry; ISO 178
 11.5 GPa
@Temperature 23.0 °C
1670 ksi
@Temperature 73.4 °F
Cond; ISO 178
Charpy Impact Unnotched 6.00 J/cm²
@Temperature 23.0 °C
28.6 ft-lb/in²
@Temperature 73.4 °F
Dry; ISO 179/1eU
Charpy Impact, Notched 0.800 J/cm²
@Temperature 23.0 °C
3.81 ft-lb/in²
@Temperature 73.4 °F
Dry; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+13 ohm-cm>= 1.00e+13 ohm-cmDry; IEC 62631-3-1
 >= 1.00e+13 ohm-cm>= 1.00e+13 ohm-cmCond; IEC 62631-3-1
Dielectric Constant  3.8
@Frequency 1e+9 Hz
3.8
@Frequency 1e+9 Hz
Dry; IEC 60250
 3.8
@Frequency 1e+10 Hz
3.8
@Frequency 1e+10 Hz
Dry; IEC 60250
 3.9
@Frequency 1e+6 Hz
3.9
@Frequency 1e+6 Hz
Dry; IEC 62631-2-1
 3.9
@Frequency 1e+6 Hz
3.9
@Frequency 1e+6 Hz
Cond; IEC 62631-2-1
 3.9
@Frequency 1e+9 Hz
3.9
@Frequency 1e+9 Hz
Cond; IEC 60250
 3.9
@Frequency 1e+10 Hz
3.9
@Frequency 1e+10 Hz
Cond; IEC 60250
 4.2
@Frequency 100 Hz
4.2
@Frequency 100 Hz
Dry; IEC 62631-2-1
 4.2
@Frequency 100 Hz
4.2
@Frequency 100 Hz
Cond; IEC 62631-2-1
Dielectric Strength 33.0 kV/mm838 kV/inDry; IEC 60243-1
 33.0 kV/mm838 kV/inCond; IEC 60243-1
Comparative Tracking Index 600 V600 VDry; IEC 60112
 >= 800 V>= 800 VSim. to IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear 35.0 µm/m-°C19.4 µin/in-°FASTM D696
 65.0 µm/m-°C36.1 µin/in-°FDry; ISO 11359-1/-2
CTE, linear, Parallel to Flow 20.0 µm/m-°C11.1 µin/in-°Fdry; ISO 11359-1/-2
 30.0 µm/m-°C16.7 µin/in-°FASTM D696
Melting Point 325 °C617 °F10°C/min. Dry; ISO 11357-1/-3
Maximum Service Temperature, Air 170 °C338 °FThermal Index; 5000 hrs.; IEC 60216/ISO 527-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 305 °C581 °FDry; ISO 75-1/-2
UL RTI, Electrical 140 °C
@Thickness 0.350 mm
284 °F
@Thickness 0.0138 in
UL746B
Flammability, UL94  V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
IEC 60695-11-10
 V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
IEC 60695-11-10

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDSM7903 / 291339

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.