MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Mocom (ALBIS) ALTECH® PE-HD A 2040/500 GF40 HDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Glass fiber Filled

Material Notes: Base Polymer: Polyethylene High Density

Filler/Additive System: 40% glass fibers

Typical Applications: Various

Information provided by Albis Plastics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.25 g/cc0.0452 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.0020 - 0.0040 cm/cm
@Time 86400 sec
0.0020 - 0.0040 in/in
@Time 24.0 hour
ISO 294-4
Linear Mold Shrinkage, Transverse 0.0080 - 0.012 cm/cm
@Time 86400 sec
0.0080 - 0.012 in/in
@Time 24.0 hour
ISO 294-4
Melt Flow 4.0 g/10 min
@Load 21.6 kg,
Temperature 190 °C
4.0 g/10 min
@Load 47.6 lb,
Temperature 374 °F
ISO 1133
Storage Temperature <= 30.0 °C<= 86.0 °Fdry, protected from light
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 30.0 MPa4350 psiISO 527
Elongation at Break 5.0 %5.0 %ISO 527
Tensile Modulus 3.10 GPa450 ksiISO 527
Flexural Strength 45.0 MPa6530 psiISO 178
Flexural Modulus 3.30 GPa479 ksiISO 178
Charpy Impact Unnotched  2.50 J/cm²
@Temperature -40.0 °C
11.9 ft-lb/in²
@Temperature -40.0 °F
ISO 179/1eU
 3.00 J/cm²
@Temperature 23.0 °C
14.3 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched  0.700 J/cm²
@Temperature -40.0 °C
3.33 ft-lb/in²
@Temperature -40.0 °F
ISO 179/1eA
 1.00 J/cm²
@Temperature 23.0 °C
4.76 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C176 °FISO 75-1/-2
Vicat Softening Point 90.0 °C194 °FB50; ISO 306
 
Processing PropertiesMetricEnglishComments
Melt Temperature 200 - 280 °C392 - 536 °FInjection molding
Mold Temperature 20.0 - 60.0 °C68.0 - 140 °FInjection molding
 
Descriptive Properties
Base PolymerPolyethylene High Density

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Alathon® M6138 High Density Polyethylene
LyondellBasell Alathon® M6060 High Density Polyethylene
Borealis MG7547S Polyethylene
Borealis Bormed™ HE7541-PH HDPE for Healthcare Applications
Total Lumicene® M6040 Metallocene High Density Polyethylene

PALBIS8299 / 242358

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.